Hastelloy Alloy C22 Polishing Sheet
video

Hastelloy Alloy C22 Polishing Sheet

Features of Hastelloy C22 polished plate
Inhibits the formation of grain boundary precipitates in the weld heat affected zone
Excellent weldability
Excellent resistance to a variety of chemical process environments, including strong oxidants such as ferric acid, acetic anhydride, seawater and brine solutions
Excellent resistance to oxidizing aqueous media
Resistant to pitting, crevice corrosion and stress corrosion cracking
Excellent resistance to reducing and oxidizing media
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy alloy c22 polishing sheet in China. If you're going to wholesale high quality hastelloy alloy c22 polishing sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

 

Hastelloy Alloy C22 Polishing Sheet Description

Hastelloy Alloy C22 Polishing Sheet

 

Gnee Steel Hastelloy Alloy C22 Polishing Sheet

Hastelloy C22 plates are key components in a wide range of industrial applications. These premium products are crafted from a low carbon nickel-based alloy that complies with ASTM B575 standards. Known for its exceptional corrosion resistance, Hastelloy C22 plates are ideal for applications that require corrosion protection.
The main alloying components of Hastelloy C22 plates include nickel, chromium, and molybdenum. As a result, USN 06022 (Nickel Alloy C22 Polished Plate) exhibits excellent creep and oxidation resistance. In addition, it maintains metallurgical stability and corrosion resistance even at elevated temperatures, making it suitable for temperatures above 540°C, like other high temperature alloy grades.
Hastelloy C22 plates are available in a variety of materials, including cold drawn plates, hot rolled plates, polished plates, and more. C22 alloy plate importers offer a comprehensive product range to meet a variety of customer needs.

Hastelloy C22 Sheets and Plate Thickness

Hastelloy C22-sheet-dimensions

Thickness
0.050 inches 1.27 mm
0.060 inches 1.524 mm
0.062 inches 1.5748 mm
0.074 inches 1.8796 mm
0.104 inches 2.6416 mm
0.093 inches 2.3622 mm
0.125 inches 3.1750 mm
0.134 inches 3.4036 mm
SURFACE FINISH THICKNESS (MM) WIDTH (MM)
2B – Cold rolled, heat-treated, pickled, skin passed 0.25–8.0 max. 2032
2D – Cold rolled, heat-treated, pickled 0.4–6.35 max. 1524
2E – Cold rolled, heat-treated, mechanically descaled 0.4–8.0 max. 2032
2R – Cold rolled, bright annealed 0.25–3.5 max. 1524
2H – Work hardened 0.4–6.35 max. 1524
Polished, brushed 0.5–4.0 max. 1524

Hastelloy C22 Sheets and Plates Specification

Specifications : ASTM B575 / ASME SB575

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length : 2000mm, 2440mm, 3000mm, 5800mm, 4000mm, etc

Thickness : 0.3 mm to 120 mm

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form : Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Chemical Composition Of Hastelloy C22 Plates

Grade C Mn Si S Co Ni Cr Fe Mo P
C22 0.010 max 0.50 max 0.08 max 0.02 max 2.50 max 50.015 min* 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 max

Hastelloy C22 Plates Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C22 8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %

Hastelloy C22 polishing Sheet Packaging

 
Hastelloy C22 polishing Sheet Packaging
 

Gnee Steel ensures the best quality of packaging, as packaging plays a vital role in international transportation, and the goods need to go through various channels to reach the final destination, so we pay special attention to packaging.

We use a variety of packaging methods depending on the product. Our product packaging methods include:

Cartons and crates
Shrink wrap
Cartons
Wooden pallets
Wooden boxes

Photo
Photo
Photo

Alloy C22 polishing Sheet Test

 

Positive material identification - PMI testing
Chemical analysis - Spectroscopic analysis
Mechanical testing, such as tensile, elongation, cross section reduction
Microscopic testing
Macroscopic testing
Hardness testing

Alloy C22 Polishing Sheet Test
Alloy C22 Polishing Sheet Test

 

Pitting resistance test
Intergranular corrosion (IGC) test
Expansion test
Flattening test
Hydrostatic pressure test
Hydrogen induced cracking (HIC) test, NACE TM0284

 

Sulfide stress corrosion cracking (SSC), NACE TM 0177
Radiographic testing
Dye penetrant testing (DP testing)
Ultrasonic testing (UT)
Eddy current testing
Impact testing
Bend testing

Alloy C22 Polishing Sheet Test

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, incoloy 825, monel alloy 400, monel k500 and high temperature alloy materials. It specializes in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automobile, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to know the alloy material price consultation or provide customized alloy material solutions, you are welcome to contact us at any time to get a quote at ss@gneesteel.com

Hot Tags: Hastelloy Alloy C22 Polishing Sheet, China Hastelloy Alloy C22 Polishing Sheet suppliers, alloy for compressors, alloy for oil and gas industry, nickel chromium iron alloy, alloy for drawing, alloy for milling, Hastelloy C

Send Inquiry

whatsapp

Phone

E-mail

Inquiry