Super Duplex S32760 Flat Bar
video

Super Duplex S32760 Flat Bar

UNS S32760 stainless steel containing 25% chromium, 7% nickel, 3.6% molybdenum as well as copper, tungsten, and nitrogen, UNS S32760 is a highly alloyed super duplex stainless steel with high PREN for use in aggressive environments.This is a super duplex grade with a ferritic-austenitic microstructure. The alloy consists of around 40-50% ferrite in the annealed condition. The super duplex microstructure has the high strength of the ferritic grades whilst retaining the corrosion resistance of the austenitic grades. It is not uncommon to see the metal used as a practical solution to chloride-induced stress cracking, which is the Achilles’ heel of stainless steel.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super duplex s32760 flat bar in China. If you're going to wholesale high quality super duplex s32760 flat bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

S32760 ss flat bar has high mechanical strength and good ductility at atmospheric temperature and sub-zero temperature, and corrosion resistance to the marine environment. Good resistance to abrasion, corrosion and cavitation, and can also be used in an acidic medium working environment.

stainless flat

Chemical Composition of ASTM A276 Super Duplex S32760 Bars:


Alloy % Ni Cr Mo N C Mn Si S P Cu W
F55 / UNS 32760,1.4501 Min 6 24 3 0.2           0.5 0.5
  Max 8 26 4 0.3 0.03 14 1 0.01 0.03 1 1

 

Physical Properties of ASTM A276 UNS S32760 Flat Bars:


Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.8 g/cm3 1350 °C (2460 °F) Psi – 80000 , MPa – 550 Psi – 116000 , MPa – 800 15 %

 

Mechanical Properties of Super Duplex Steel UNS S32760 Flat


Room temperature mechanical properties

UNS S32760

0.2% yield strength (N/mm 2 ) Tensile strength (N/mm 2 ) Elongation (%) Hardness (HB) Impact energy
at room temperature, V-notch, actual size (J)
≧ 550 ≧ 750 ≧ 25 ≦ 270 ― ―

EN 1.4501

0.2% yield strength (N/mm 2 ) Tensile strength (N/mm 2 ) Elongation (%) Hardness (HB) Impact energy
at room temperature, V-notch, actual size (J)
≧ 530 730-930 ≧ 25 ― ≧ 100 (long) ≧ 60 (tr)

 

UNS S32760 Stainless Flat Bar can be used in a variety of applications including:

Desalination plants

Seawater systems

Heat exchangers

Subsea pipework systems

Flue gas desulphurisation (FGD) plants

Centrifuges and agitators

Valves and pumps

Storage tanks and pressure vessels

 

Customer Visit

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

GNEE

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: super duplex s32760 flat bar, China super duplex s32760 flat bar suppliers, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry