Stainless Steel Bar S34700, Stainless Steel Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel bar s34700, stainless steel bar in China. If you're going to wholesale high quality stainless steel bar s34700, stainless steel bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel Bar S34700, Stainless Steel Bar
Product Description
Company Profile
1.SGS and BV Audited company.
2.Industry experience over 20 years.
3.Management Systems-Internal Software
4.Finished Product Inventory-More Than 500 Tons.
5.Raw Material inventory -Over 800 Mertic Tons.
6.Shipment of goods -More than 50 countries worldwide.
7.We have the most convenient transport and prompt delivery.
8.We offer competitive price with best service.
9.We have high technical production line with top quality products.
10.We have win high reputation based on best quality products.
We provide Stainless Steel Plate, Stainless Steel Tube,Stainless Steel Barr
Standard: ASTM, JIS, DIN, AISI, KS, EN, etc.
Type: 201, 202, 304, 304L, 309S, 310S, 310H , 314 ,316, 316L, 316Ti, 317, 317L, 347, 347H , 321, 403 , 405 ,409, 409L, 410 , 410L , 420, 429 , 430, 434 ,444, 904L , 2014 and 2205 ,Uranus 65 ,C126
Martensite-Ferritic: Ss 405 , 409, 409L, 410, 420, 420J1 , 420J2 , 420F , 430 ,431 sheet / plate;
Austenite Cr-Ni -Mn: Ss 201 sheet, ss 202 sheet, J4 ss coil;
Austenite Cr-Ni: SS 304 sheet, SS 304L sheet, ss 309S sheet, ss 310S plate;
Austenite Cr-Ni -Mo: Stainless steel 316 plate, stainless steel 316L plate;
Super Austenitic: 904L Stainless steel sheet , 2205 stainless steel sheet ,253MA stainless steel plate 254SMO stainless steel plate , 654MO stainless steel Plate,
Duplex : S32304 , S32550 ,S31803 ,S32750
EN Standard:
Austenitic: 1.4372 ,1.4373, 1.4310, 1.4305, 1.4301, 1.4306 , 1.4318 ,1.4335, 1.4833 , 1.4835 , 1.4845, 1.4841, 1.4401 , 1.4404 , 1.4571 ,1.4438, 1.4541 , 1.4878 , 1.4550 , 1.4539 , 1.4563 , 1.4547
Duplex: 1.4462 , 1.4362 ,1.4410 , 1.4507
Ferritic :1.4512, 1.400 , 1.4016 ,1.4113 , 1.4510 ,1.4512, 1.4526 ,1.4521 , 1.4530 , 1.4749 ,1.4057;
Martensitic: 1.4006 , 1.4021 ,1.4418 ,S165M ,S135M;
CHEMICAL COMPOSITION
| Company | Tianjin Yitejia Steel Sales Co., Ltd | ||
| Grade | Compositionnominal wt% | Elongation % | Hardness |
| 301 Annealed 1/4H 1/2H FH | C .15, Mn 2.0, P .045, S 0.3, Si .75, Cr 16-18, Ni 6-8, N .1 | 40 | 95 Rb |
| 302 | C 0.15, Mn 2.0, P .045, S .03, Si .75 Cr 17-19, Ni 8-10, N .1 | 40 | 92 Rb |
| 303 | C 0.15, Mn 2.0, P .045, S .03, Si .75 Cr 17-19, Ni 8-10, N .1 | 30-50 | 92 Rb |
| 304 | C .08, Mn 2.0, P .045, S .03, Si .75 Cr 18-20, Ni 8-10.5, N .10 | 40 | 92 Rb |
| 304L | C .03, Mn 2, P .045, S .03, Si .75, Cr 18-20, Ni 8-12, N .1 | 40 | 92 Rb |
| 305 | C .12, Mn 2.0, P .045, S .03, Si .75, Cr 17-19, Ni 10.5-13, | 40 | 88 Rb |
| 309/309S | Type 309 - C .2, Mn 2.0, P .045, S.03, Si .75 Cr 22-24, Ni 12-15, Fe bal Type 309S - C .08, Mn 2.0, P .045, S .03, Si. 75, Cr 22-24, Ni 12-15, Fe Bal | 49/ 44.6 | - |
| 310L | Mn 1.10, Cr 24.5, Ni 20.5 (nominal) | 40 | 95 Rb |
| 310 310S | 310: C .25, Mn 2, P 0.045, S 0.03, Si 1.5, Cr 24-26, Ni 19-22, Fe balance 310S: C 0.08, Mn 2, P 0.045, S 0.30, Si 1.5, Cr 24-26, Ni 19-22, Fe balance | 45/42/6 | - |
| 316 | C .08, Mn 2.0, Si .75, Cr 16-18, Ni 10-14, Mo 2-3, P .045, S .03, N .1, Fe Bal | 40 | 95 Rb |
| 316L | C .03, Mn 2.0, Si .75, Cr 16-18, Ni 10-14, Mo 2-3, P .045, S .03, N 0.1, Fe Bal | 54 | 95 Rb |
| 316Ti | C .08, Mn 2.0, Si .75, Cr 16-18, Ni 10-14, Mo 2-3, P 0.045, S 0.03, N 0.1, Ti 0.15-0.70, balance Fe | 248 | 76 Rb |
| 317 | Type 317 - C .08, Mn 2.0, Si .75, Cr 18-20, Ni 11-15, Mo 3-4, P .045, S .03, N .10, Fe Bal | 35 | 95 Rb |
| 321 | C .09, Mn 2.0, P .045, S .03, Si .75, Cr 17-18, Ni 9-12, Ti .7, N .1 Fe Bal | 40 | 95 Rb |
| 334 | C 0.03, Mn 1.0, P .02, S .015, Si .75, Cr 19-19.5 Ni 19-20, Ti .4, Al .4, Cu .2 Fe Bal | 40 | 82 Rb |
| 347 | C .08, Mn 2.0, P .045, S .03, Si .75, Cr 17-19, Ni 9-13, Cb+Ta 1.0, Fe Bal | 40 | 95 Rb |
| 348 | C .08, Mn 2.0, P .045, S .03, Si.75, Cr 17-19, ni 9-13, Cb+Ta 1.0, Ta .10, Co .2, Fe Bal | 40 | 92 Rb |
| 410 | C .15, Mn 1.0, Si 1.0, Cr 11.5-13.5, Ni 0.5, S .03, Ph .04 | 34 | 38-45 Rc |
| 416 | C 0.15, Mn 1.25, Si 1.0, Cr 12-14, P 0.06, S 0.15, Mo 0.60, Fe Balance | 15-30 | |
| 420 | C .15-.40, Mn 1.0, Si 1.0, Cr 12-14, Ni 0.5, S .03, Ph .04 | 15-30 | 53-57 Rc |
| 440A | C .60-.75, Mn 1.0, Si 1.0, Cr 16-18, Mo .75, Ni .50, S.03, Ph .04 | 20 | 57-60 Rc |
| 440C | Cr 16.5, C 1.0, Si 1.0 | - | 58 Rc |
| 13-8 Mo | Cr 13, Ni 8, Mo 2, Al, low C, balance Fe | 18 | 33 Rc |
| 15-5PH | Cr 15, Ni 5, Cu 3, Cb, balance Fe | 10 | 33 Rc |
| 15-7Mo | Cr 15, Ni 7, Mo 2, AL 1, balance Fe | 30 | 88 Rb |
| 17-4PH | Cr 17, Ni 4,Cu 3, Cb, balance Fe | 8 | 33 Rc |