20Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420
video

20Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420

Stainless steel 410/420, also known as UNS S41000 and UNS S42000, is considered a basic martensitic stainless steel. Comprised of 11.5% to 13.5% chromium and iron, along with trace amounts of other elements including carbon, manganese, phosphorus, silicon, and sulfur. After heat treatment, Stainless Steel 410 exhibits high mechanical properties, it is magnetic in both hardened and annealed conditions.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 20cr13 od 170mm stainless steel round bar forged shaft rod astm a276 420 in China. If you're going to wholesale high quality 20cr13 od 170mm stainless steel round bar forged shaft rod astm a276 420 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

20Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420

Description

Certification: ISO,BV,SGS Surface: Bright
Outdiameter: 4-100mm Length: 4-10m
Grade: 201 301 304 316L Type: Round
Application: Construction Standard: ASTM
Grade: 400 Series 420 Shape: Round
Dimensions: 5.5mm-500mm Packing: Standard Seaworthy Package
Price Term: CIF CFR FOB Ex-Work
High Light:

Stainless Steel Round Bar Forged Rod

,

OD 170mm Stainless Steel Round Bar

,

A276 420 Stainless Steel Round Bar

410/420 Stainless Steel Bar

UNS S41000/UNS S42000

Stainless steel 410/420, also known as UNS S41000 and UNS S42000, is considered a basic martensitic stainless steel. Comprised of 11.5% to 13.5% chromium and iron, along with trace amounts of other elements including carbon, manganese, phosphorus, silicon, and sulfur. After heat treatment, Stainless Steel 410 exhibits high mechanical properties, it is magnetic in both hardened and annealed conditions. Upon specification, Stainless Steel 410 can be delivered in a hardened, yet still machinable state for uses where moderate corrosion resistance and high strength are required. Stainless Steel 410 reaches maximum corrosion resistance when hardened, tempered and polished. It can be welded using most common welding methods, hot worked between 2000° F and 2200° F, as well as, cold formed and annealed. Because of all of these traits it is widely considered the "general purpose grade" of stainless steel.

UNS S42000, commonly known as Stainless Steel 420 is the high carbon content version of Stainless Steel 410. Corrosion resistance is similar between the two, but Stainless Steel 420 additionally provides increased strength and hardness. Like Stainless Steel 410 it is also considered a "general purpose grade" including at least 12% chromium, which is enough to give it acceptable corrosion resistance. Typically, Stainless Steel 420 achieves its best corrosion resistance when the alloy is hardened and polished, or surface ground.

Industries that use 410 & 420 include:

Automotive

Dental/Medical

Electrical

Food processing

Forging

Petrochemical

Tool

Tractor

Products partially or completely constructed of 410 & 420 include:

Bearings

Bushings

Cutlery

Dies

Fasteners

Hand tools

Plastic molds

Pump shafts

Screens

Steam/Gas

Surgical instruments

Turbine blades

Valves/Valve components

410 COND A STOCKING DIAMETERS 1/2" TO 16"
MATERIAL LENGTHS UP TO 24'
410 COND HT ASTM A-479 COND 2 STRESS RELIEVED STOCKING DIAMETERS 1/2" TO 7"
MATERIAL LENGTHS UP TO 24'
420 COND A STOCKING DIAMETERS 1/2" TO 14"
MATERIAL LENGTHS UP TO 24'
BAR SPECIFICATIONS
UNS TYPE AMS ASTM FEDERAL CHARACTERISTICS
S41000 410 5613 A-276
A-314
A-479
A-493
QQ-S-763 410 is a low cost general purpose stainless steel, that hardens at 35-39 RC and is used widely where corrosion is not severe.
S42000 420 5621 A-276
A-314
QQ-S-763 420 is similar to 400, but the raised carbon content produces higher strength and hardness. Heat treatment to 50 RC min.
CHEMISTRY ANALYSIS – 410
C MN P S SI CR NI MO CU OTHER M/NM
0.15 1.0 0.04 0.03 1.0 11.5 – 13.5 0.75 0.5 0.5 Al .05
Sn .05
N .08
M
CHEMISTRY ANALYSIS – 420
C MN P S SI CR NI MO CU OTHER M/NM
0.15 Min. 1.0 0.04 0.03 1.0 12. 0– 14.0 0.5 0.5 0.5   M

 

RESISTANCE

Corrosion Resistance:

Less resistant than the austenitic grades and the 17% chromium ferritic alloys

Good resistance in the hardened condition to the atmosphere, foods, fresh water, and mild acids

Resistance lowered in the annealed condition

Best with a smooth surface finish

Heat Resistance:

Not recommended for use above the relevant tempering temperature because of reduction in mechanical properties

Scaling temperature is approximately 1202oF (650oC)

 

PROCESSING

 

Machinability

Tough, stringy chip build-up.

Similar to machining some of the high carbon tool steel

Welding

Not commonly welded due to air hardening characteristics.

Welding may be performed after preheating to 300-400 F

Post weld tempering at temperature for 2 hours

Hot Working

Recommended to bring temperatures slowly up to 1400, then on to 2000-2200 F

Furnace cool slowly to avoid cracking, after furnace working

Reheating is necessary to keep working temperature above 1600 F.

Cold Working

Can withstand only minor cold work.

Radical forming operations will result in cracking.

Annealing

Anneal at temperatures between 1550-1650 F (843-900 C)

Allow for slow furnace cooling.

Tempering

Temper at temperatures of 300-400 F

Air cool for maximum hardness and corrosion resistance.

Hardening

Soak at 1850-1950 F to quench in heated oil.

20Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420 020Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420 1

20Cr13 OD 170mm Stainless Steel Round Bar Forged Shaft Rod ASTM A276 420 2

Hot Tags: 20cr13 od 170mm stainless steel round bar forged shaft rod astm a276 420, China 20cr13 od 170mm stainless steel round bar forged shaft rod astm a276 420 suppliers, 304 304L 316 316L Stainless Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry