S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate
video

S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate

S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate Description Width: 600-2500mm Grade: S355J2+N Technique: Hot Rolled Type: Steel Plate Standard: ASTM,AISI,JIS,DIN Length: 1000-12000mm Special Use: High-strength Steel Plate Thickness: 6-100mm Product Name: High Quality S355J2+N Hot Rolled Carbon Steel Plate Shape: Flat Steel Plate High Light: 10mm Hot Rolled Carbon Steel Plate , 1.0577 Hot Rolled Carbon Steel Sheet , S355J2+N Hot Rolled Mild Steel Sheet
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s355j2+n 10*1500*3000mm 1.0577 steel plate hot rolled products of structural steel en 10025-2 3.1 certificate in China. If you're going to wholesale high quality s355j2+n 10*1500*3000mm 1.0577 steel plate hot rolled products of structural steel en 10025-2 3.1 certificate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate

Description

Width: 600-2500mm Grade: S355J2+N
Technique: Hot Rolled Type: Steel Plate
Standard: ASTM,AISI,JIS,DIN Length: 1000-12000mm
Special Use: High-strength Steel Plate Thickness: 6-100mm
Product Name: High Quality S355J2+N Hot Rolled Carbon Steel Plate Shape: Flat Steel Plate
High Light:

10mm Hot Rolled Carbon Steel Plate

,

1.0577 Hot Rolled Carbon Steel Sheet

,

S355J2+N Hot Rolled Mild Steel Sheet

S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products of Structural Steel EN 10025-2 3.1 Certificate

 

S355J2 Steel (Material 1.0577)

S355J2 steel (1.0577) is a quality grade of S355 steel, which is one of the non-alloy structural steels commonly used in Europe. According to EN 10025-2: Hot rolled products of structural steels, S355 steel is divided into 4 quality grades, namely:

S355JR (1.0045),

S355J0 (1.0553),

S355J2 (1.0577), former names: S355J2G3 and S355J2G4 in EN 10025:1990,

S355K2 (1.0596), previous names: S355K2G3 and S355K2G4 in EN 10025:1990.

EN 10025 S355J2 equivalent ASTM A992/A992M; Australian AS/NZS 3678: Grade 350 L20; Canadian G40.20/G40.21: 350WT (55WT); Chinese GB/T 1591: Q355D; and Indian standard IS 2062: E350.

EN 10025 S355J2 Meaning

S355J2 Meaning: "S" stands for "Structural steel"; 355 indicates that the material has a minimum yield strength of 355 MPa when the nominal thickness is ≤ 16mm; and "J2" indicates that the material has a minimum impact energy of 27J at -20°C (-4 °F).

S355J2 Steel Properties

S355J2 steel properties are listed in the datasheet below, including chemical composition, physical and mechanical properties, etc.

Chemical Composition

Chemical composition based on heat analysis.

Chemical Composition, % (≤)
Standard Steel (Material Number) C Si Mn P S Cu N Method of deoxidation
EN 10025-2 S355J2 (1.0577) 0.20 0.55 1.60 0.025 0.025 0.55 – Fully killed

Note: For carbon content (C) and nominal thickness (t)

C ≤ 0.20 % when t ≤ 16mm,

C ≤ 0.22 % when t > 30 mm,

C by agreement when sections with nominal thickness > 100 mm.

For long products the P and S content can be 0.005 % higher.

Chemical Composition (Product Analysis), % (≤)
Standard Steel (Material Number) C Si Mn P S Cu N Method of deoxidation
EN 10025-2 S355J2 (1.0577) 0.23 0.6 1.70 0.035 0.035 0.60 – Fully killed

Note: For carbon content (C) and nominal thickness (t)

C ≤ 0.23 % when t ≤ 16mm,

C ≤ 0.24 % when t > 30 mm,

C by agreement when sections with nominal thickness > 100 mm.

For long products the P and S content can be 0.005 % higher.

Mechanical Properties

S355J2 mechanical properties at room temperature are listed in the datasheet below, including tensile strength, yield strength, and elongation, etc.

Yield Strength, Mpa, ≥
Steel Grade (Steel Number) t≤16 16< t ≤40 40< t ≤63 63< t ≤80 80< t ≤100 100< t ≤150 150< t ≤200 200< t ≤250 250< t ≤400
S355J2 (1.0577) 355 345 335 325 315 295 285 275 265
Tensile Strength, Mpa, ≥
Steel Grade (Material Number) t<3 3 ≤ t ≤ 100 100 < t ≤400
S355J2 (1.0577) 510-680 470-630 450-600

Note:

1 MPa = 1 N/mm2

t = Nominal Thickness (mm)

S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate 0S355J2+N 10*1500*3000mm 1.0577 Steel Plate Hot Rolled Products Of Structural Steel EN 10025-2 3.1 Certificate 1

Hot Tags: s355j2+n 10*1500*3000mm 1.0577 steel plate hot rolled products of structural steel en 10025-2 3.1 certificate, China s355j2+n 10*1500*3000mm 1.0577 steel plate hot rolled products of structural steel en 10025-2 3.1 certificate suppliers, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry