S17700 17-7 PH AISI 631 Stainless Steel Round Bar Stock 260mm
video

S17700 17-7 PH AISI 631 Stainless Steel Round Bar Stock 260mm

17-7 PH is a chromium-nickel-aluminum precipitation hardening stainless steel that provides high strength and hardness and a moderate level of corrosion resistance up to 600˚F. This grade can be easily formed in the austenitic condition similar to Type 301 stainless steel and hardened to high strength levels using relatively low heat treatments that minimize distortion. The corrosion resistance of 17-7 PH is comparable to that of Type 304 stainless steel, especially in the CH 900 temper, and it has been used for spring applications, washers, eyelets, fittings and fasteners.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s17700 17-7 ph aisi 631 stainless steel round bar stock 260mm in China. If you're going to wholesale high quality s17700 17-7 ph aisi 631 stainless steel round bar stock 260mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Stainless Steel PH 17-7 Material Round Bar Ø260 ASTM S17700 AISI631,SAE17-7PH Forge Rod

 

17-7 PH is a chromium-nickel-aluminum precipitation hardening stainless steel that provides high strength and hardness and a moderate level of corrosion resistance up to 600˚F. This grade can be easily formed in the austenitic condition similar to Type 301 stainless steel and hardened to high strength levels using relatively low heat treatments that minimize distortion. The corrosion resistance of 17-7 PH is comparable to that of Type 304 stainless steel, especially in the CH 900 temper, and it has been used for spring applications, washers, eyelets, fittings and fasteners.

Heat treatments can strengthen this type of stainless steel. The typical process for 17-7 PH heat treatment has three or four steps:

Conditioning using austenite.

Cooling, which turns the austenite into martensite.

Precipitation hardening until Condition TH 1050 or RH 950 has been reached.

To achieve the highest mechanical properties Condition A material is transformed to martensite at the mill by cold reduction to Condition C. After fabrication by the user, a single low-temperature heat treatment is preformed to achieve condition CH 900.

Chemical Composition

 

Element Content(%)
Chromium, Cr 16-18
Nickel, Ni 6.50 – 7.75
Manganese, Mn 1 max
Silicon, Si 1 max
Aluminum, Al 0.75 – 1.50
Carbon, C 0.09 max
Phosphorous, P 0.040 max
Sulfur, S 0.030 max
Iron, Fe balance

 

Physical Properties

 

 

Properties Metric Imperial
Density 7.80 g/cm3 0.282 lb/in3
Melting Range 1404-1440°C 2560-2625°F

 

 

Mechanical Properties

 

Properties Metric Imperial
Tensile Strength 1170 MPa 170000 psi
Yield Strength 965 MPa 14000 psi
Modulus of Elasticity 204 GPa 29600 ksi
Poisson's Ratio 0.27-0.30 0.27-0.30
Elongation at Break 6% 6%
Hardness, Rockwell C 38 38

 

S17700 17-7 PH AISI 631 Stainless Steel Round Bar Stock 260mm 0S17700 17-7 PH AISI 631 Stainless Steel Round Bar Stock 260mm 1

Hot Tags: s17700 17-7 ph aisi 631 stainless steel round bar stock 260mm, China s17700 17-7 ph aisi 631 stainless steel round bar stock 260mm suppliers, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes

Send Inquiry

whatsapp

Phone

E-mail

Inquiry