Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T
video

Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T

18CrNiMo7-6 round Bar – Case-Hardened Steel mainly used in mechanical parts, automobile parts, cement plants, power plants, mobile cranes and earth-moving equipment, paper mill, sugar mill, marine, wind gear, oil platform, fire protection, medical fields, industry equipment, collets, cams, rollers, bushes, spindles, and gears, etc.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy steel round bar rod din 18crnimo7-6 1.6587 solution annealing q+t in China. If you're going to wholesale high quality alloy steel round bar rod din 18crnimo7-6 1.6587 solution annealing q+t made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T

Description

Steel Grade: Alloy Steel Alloy Or Not: Is Alloy
Technique: Hot Rolled,Forged Application: Tool Steel Bar
Type: Alloy Steel Bar,Mold Steel,high Speed Tool Steel Standard: ASTM,DIN,AISI,JIS
Shape: Round Length: 1--12m
Surface Treatment: Black/Peeling/Polishing/Machined Diameter: 12mm-650mm
Delivery Condition: Annealed,hot Rolled/forged Dimensions: 5-900MM
Heat Treatment: Normalized +Annealed +Quenched + Tempered
High Light:

Solution Annealing Steel Round Bar Rod

,

900MM Steel Round Bar Rod

,

Steel Round Bar Rod 650mm

17CrNiMo7-6 Alloy Steel Round Bar DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T Alloy Rod

18CrNiMo7-6 Round Bar – Case-Hardened Steel – Din 17210 EN 10084

Application

18CrNiMo7-6 round Bar – Case-Hardened Steel mainly used in mechanical parts, automobile parts, cement plants, power plants, mobile cranes and earth-moving equipment, paper mill, sugar mill, marine, wind gear, oil platform, fire protection, medical fields, industry equipment, collets, cams, rollers, bushes, spindles, and gears, etc.


Quality Standard

-BS EN 10084-2008 Case hardening steels.

-DIN 17210 for Case hardening steel.


Steel Grades

EN DIN ANFOR

18CrNiMo7-6 1.6587 18NCD6


Chemical Composition(%)

C Si Mn P S Cr Mo Ni
0.15-0.21 0.40 max 0.50-0.90 0.025 max 0.025 max 1.50-1.80 0.25-0.35 1.40-1.70

Mechanical Properties

Process Tensile Strength Rm (Mpa) Yield Strength Rp0.2 (Mpa) Elongation A5 (%) Area Reduction Ratio C (%) Hardness (HB)
Annealed / / / / 229 max
Normalized / / / / 140-210
Q+T 980-1270 685 min 8 min 35 min 295-373

Heat Treatment
Annealing: Heat 18CrNiMo7-6 to 650-700°C, cool slowly in furnace.
Normalizing: 850-880°C, air.
Hardening: Carburising: 880-980°C. Core Hardening: 830-870°C, water. Case Hardening: 780-820°C, water.
Tempering: 150-200°C.


Capacity

3,000 ton per month.


Test

Chemical analysis, Mechnical analysis, Ultrasonic testing, Metallographic, Surface quality and dimension report.


Package

Each bundle of max 3,000kg with several steel strips, Two tags on each bundle, Wrapped in waterproof paper, PVC sleeve, and sackcloth with several steel strips.


Mill's Test Certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T 0Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T 1Alloy Steel Round Bar Rod DIN 18CrNiMo7-6 1.6587 Solution Annealing Q+T 2

Hot Tags: alloy steel round bar rod din 18crnimo7-6 1.6587 solution annealing q+t, China alloy steel round bar rod din 18crnimo7-6 1.6587 solution annealing q+t suppliers, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes

Send Inquiry

whatsapp

Phone

E-mail

Inquiry