38CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm
video

38CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm

The process flow of nitriding parts is generally: forging → normalizing (annealing) → rough machining → tempering and tempering → finishing machining → de-stress → fine grinding → nitriding → fine grinding → assembly. The purpose of 38CrMoAl nitriding treatment is mainly for wear resistance.After nitriding, its hardness is as high as HV800, the hardened layer can reach 0.30mm ~ 0.5mm.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 38crmoal alloy structure steel round bar din 1.8509 41cralmo7-10 forged rod 650mm in China. If you're going to wholesale high quality 38crmoal alloy structure steel round bar din 1.8509 41cralmo7-10 forged rod 650mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

38CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm

Description

Steel Grade: Alloy Steel Alloy Or Not: Non-alloy
Technique: Hot Rolled,Forged Application: Structural Steel Bar
Type: Alloy Steel Bar Standard: ASTM,DIN,GB,AISI,JIS
Shape: Round Length: 1--12m
Surface: Black Or Bright Diameter: 12mm-650mm
Delivery Condition: Annealed Heat Treatment: Normalized +Annealed +Quenched + Tempered
High Light:

Alloy Steel Round Bar Forged Rod

,

38CrMoAl Steel Round Bar Rod

,

Alloy Steel Round Bar Rod 650mm

38CrMoAl Alloy Structure Steel (Nitride Steel) Round Bar DIN 1.8509 41CrAlMo7-10 Forged Steel Rod

38CrMoAl is an alloy structural steel characterized by high aluminum composition, which is generally used after quenching and nitriding.After nitriding, 38CrMoAl has high surface hardness, wear resistance and fatigue strength, and has good heat resistance and corrosion.

The characteristic of 38CrMoAl nitriding is that the speed is fast and the depth of nitriding layer can be obtained. However, the brittleness of the nitriding layer is relatively large, so it is not suitable for making parts that bear great impact.

 

CHEMICAL COMPOSITION(%)

STANDARD GB/T 3077 SAE 6470 JIS G4053 DIN EN 10085
GRADE 38CrMoAl

135 Mod

UNS K24065

SACM645

(SACM1)

1.8509

41CrAlMo7-10

C 0.35~0.42 0.38~0.43 0.40~0.50 0.38~0.45
Si 0.20~0.45 0.20~0.40 0.15~0.50 ≤0.40
Mn 0.30~0.60 0.50~0.80 ≤0.60 0.40~0.70
P ≤0.035 ≤0.025 ≤0.030 ≤0.025
S ≤0.035 ≤0.025 ≤0.030 ≤0.035
Cr 1.35~1.65 1.40~1.80 1.30~1.70 1.50~1.80
Mo 0.15~0.25 0.30~0.40 0.15~0.35 0.20~0.35
Al 0.70~1.10 0.95~1.30 0.70~1.20 0.80~1.20

 

HEAT TREATMENT

TYPES TEM ℃ COOLING HRC
ANNEALING 840~870 FURNACE COOLING ≤229HB
NORMALIZING 930~970 AIR COOLING -
QUENCHING 940 OIL >56
TEMPERING 150~200 WATER OR OIL 51~56
300~400 WATER OR OIL 45~51
500~550 WATER OR OIL 35~39
600~650 WATER OR OIL 28~31

 

TRIDING TREATMENT

The process flow of nitriding parts is generally: forging → normalizing (annealing) → rough machining → tempering and tempering → finishing machining → de-stress → fine grinding → nitriding → fine grinding → assembly.

The purpose of 38CrMoAl nitriding treatment is mainly for wear resistance.After nitriding, its hardness is as high as HV800, the hardened layer can reach 0.30mm ~ 0.5mm.

 

APPLICATION

38CrMoAl is mainly used in the manufacture of parts with precise size, requiring high wear resistance and fatigue strength, and not subjected to large impact load, such as cylinder liner, bottom sleeve, gear, bolts, shaft and rotor, etc.

In addition, because Al and Cr elements can form a dense passivation film on the surface of steel, so 38CrMoAl is also a kind of seawater corrosion resistant steel.Its seamless steel pipe is the most ideal pipeline and processing material for transporting water, oil and gas and seawater containing medium in coastal power plants, coastal oil fields, coastal natural gas and petrochemical plants.

 

38CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm 038CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm 138CrMoAl Alloy Structure Steel Round Bar DIN 1.8509 41CrAlMo7-10 Forged Rod 650mm 2

Hot Tags: 38crmoal alloy structure steel round bar din 1.8509 41cralmo7-10 forged rod 650mm, China 38crmoal alloy structure steel round bar din 1.8509 41cralmo7-10 forged rod 650mm suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes