17-4 PH Stainless Steel Flat Bar
video

17-4 PH Stainless Steel Flat Bar

Our stainless steel bar stock lengths range from the industry standard 12' to 28' long. For projects requiring long-length stainless steel bar, our inventory ranges from 20’-28’ R/L. We also offer several shape options, including pump shafts, round bar, square bar, boat shafts, flat bar, and hex bar shapes.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 17-4 ph stainless steel flat bar in China. If you're going to wholesale high quality 17-4 ph stainless steel flat bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Our 17-4 PH Stainless Steel (SS) is a precipitation-hardening martensitic stainless steel, with a chemical makeup of approximately 17% chromium and 4% nickel. Typical usage is seen in applications requiring high strength and an excellent level of corrosion resistance. The strength and toughness desired can be manipulated by the temperate range in the heat treatment process. GNEE Steel offers high-quality standards of 17-4 stainless steel bar including UNS S17400, AMS 5643, ASTM A564, and ASTM A693 Grade 630.

ss flat bar

stainless-steel-flat-bar

 

17-4 PH SS Flat Bar Composition

Carbon 0.070 max

Chromium 15.00 - 17.50

Columbian + Tantalum 0.15 - 0.45

Copper 3.00 - 5.00

Manganese1.00 max

Nickel 3.00 - 5.00

Phosphorus 0.040 max

Silicon 1.00 max

Sulfur 0.030 max

 

17-4 PH Stainless Steel Flat Bar Applications

  • Pump Shafts
  • Oil Patch
  • Mechanical Seals
  • Aerospace

 

Customer Visit 

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

gnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: 17-4 ph stainless steel flat bar, China 17-4 ph stainless steel flat bar suppliers, Stainless Steel 446 Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry