Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040
video

Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040

Ultimate tensile strength is the maximum load a material will support before it breaks, explains Instron, a materials testing laboratory. Ultimate tensile strength testing is a destruction test. The purpose is to find the point at which a material will fail when supporting a given load or sustaining a set force.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of wear resistant carbon steel plate 10mm 2000*6000mm material c-1040 in China. If you're going to wholesale high quality wear resistant carbon steel plate 10mm 2000*6000mm material c-1040 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040

Description

Width: 600-2500mm Grade: Q235,Q345,SS400
Application: Boiler Plate Technique: Hot Rolled,Cold Rolled
Type: Steel Plate,Steel Sheet Standard: ASTM,GB,AISI,JIS,DIN
Length: 1000-12000mm Special Use: High-strength Steel Plate,Wear Resistant Steel,Industry Construction,Pressure Vessel Boiler
Thickness: 6-400mm Shape: Flat Steel Plate
High Light:

Wear Resistant Carbon Steel Boiler Plate

,

2000*6000mm Carbon Steel Plate

,

C-1040 Carbon Steel Plate

Product Details

Physical Properties  
Density (lb / cu. in.) 0.284
Specific Gravity 7.86
Specific Heat (Btu/lb/Deg F - [32-212 Deg F]) 0.107
Melting Point (Deg F) 2770
Poissons Ratio 0.3
Thermal Conductivity 360
Mean Coeff Thermal Expansion 6.7
Modulus of Elasticity Tension 30
Modulus of Elasticity Torsion 11

 


CARBON 1040 STEEL STRUCTURAL PLATE- Used when greater strength and hardness is desired in the as rolled condition. Good for hammer forge processes. Uses include gears, shafts, axles, bolts sand studs. 1040 is a medium-carbon steel composed of 0.37 to 0.44 percent carbon, 0.6 to 0.9 percent manganese, a maximum of 0.04 percent phosphorus and a maximum of 0.05 sulphur. The remainder is iron. 1040 steel sometimes contains 0.1 to 0.35 percent silicon, according to Interlloy, an Australia-based alloy engineering steel, tool steel and specialty steel producer.

CARBON 1040 STEEL STRUCTURAL PLATE equivalent to EN8/080M40. An unalloyed medium carbon steel. AISI 1040 is a medium strength steel with good tensile strength. Suitable for shafts, stressed pins, studs, keys etc. 1040 must be pre-heated to 300 to 500 degrees F before welding and reheated to between 1100 degrees F and 1200 degrees F after welding. Otherwise, the area near the weld may develop cracks or become brittle and cause the part to fail during use.

Tensile Strength
Ultimate tensile strength is the maximum load a material will support before it breaks, explains Instron, a materials testing laboratory. Ultimate tensile strength testing is a destruction test. The purpose is to find the point at which a material will fail when supporting a given load or sustaining a set force.

CARBON 1040 STEEL STRUCTURAL PLATE will support 90,000 pounds of force per square inch before it fails, if it was hot-rolled. This strength drops to 85,500 psi when the steel has been normalized, or returned as closely as possible to the state it was in when it was produced. Tensile strength drops even further, to 72,250, when it has been annealed, or brought to its softest point while cold.

Normalizing and annealing are two examples of heat treatments. In heat treatment the temperature of the steel is changed in order to alter its molecular structure and change its reaction to various forces during forging and fabrication, according to metallurgist David Pye's heat treatment tutorial at Moldmaking Technology.

 

Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040 0Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040 1Wear Resistant Carbon Steel Plate 10Mm 2000*6000mm Material C-1040 2

Hot Tags: wear resistant carbon steel plate 10mm 2000*6000mm material c-1040, China wear resistant carbon steel plate 10mm 2000*6000mm material c-1040 suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet, Stainless Steel 316 316L 316Ti Sheets And Plates, 1 4510 Stainless Steel Patterned Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry