ASTM A204 Alloy Steel Plate 100mm Thickness 16Mo3 Molybdenum
video

ASTM A204 Alloy Steel Plate 100mm Thickness 16Mo3 Molybdenum

Specifications for 16Mo3 Sheets & Plates. If any specification is not mentioned here, please use the contact button for quick quote. Specifications ASTM A204 / ASME SA204 Standard AISI, ASTM, BS, DIN, GB, JIS Thickness 4.0mm – 100mm Specialize Shim Sheet, Perforated Sheet, B. Q. Profile. Length 1000-12000 mm Form Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. Grade ASTM A204 16MO3
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a204 alloy steel plate 100mm thickness 16mo3 molybdenum in China. If you're going to wholesale high quality astm a204 alloy steel plate 100mm thickness 16mo3 molybdenum made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

16Mo3 Sheets & Plates Specifications

Specifications for 16Mo3 Sheets & Plates. If any specification is not mentioned here, please use the contact button for quick quote.

Specifications ASTM A204 / ASME SA204
Standard AISI, ASTM, BS, DIN, GB, JIS
Thickness 4.0mm – 100mm
Specialize Shim Sheet, Perforated Sheet, B. Q. Profile.
Length 1000-12000 mm
Form Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange)
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Grade ASTM A204 16MO3

Types of 16Mo3 Sheets & Plates

 

ASTM 16Mo3 Steel Polished Sheets

WERKSTOFF NR. 1.5415 Polished Sheets

ASTM 16Mo3 Steel Hot Rolled Sheets

ASTM 16Mo3 Steel Cold Rolled Sheets

ASTM 16Mo3 Steel Sheets

ASTM 16Mo3 Steel Shim Sheets

ASTM 16Mo3 Steel Perforated Sheets

ASTM 16Mo3 Steel Class 1 Sheets

ASTM 16Mo3 Steel Plates

 

 

WERKSTOFF NR. 1.5415 Hot Rolled Plates

ASTM 16Mo3 Steel Checkered Plates

ASTM 16Mo3 Steel Cold Rolled Plates

WERKSTOFF NR. 1.5415 Cold Rolled Plates

ASTM 16Mo3 Steel Polished Plates

WERKSTOFF NR. 1.5415 Polished Plates

ASTM 16Mo3 Hot Rolled Plates

ASTM 16Mo3 Steel Cold Rolled Plates

ASTM 16Mo3 Steel Class 1 Plates

 

 

16Mo3 Sheets & Plates Chemical Composition

Grade min max
C 0.12 0.2
Cu – 0.30
N – 0.012
Mn 0.40 0.90
Mo 0.25 0.35
P – 0.025
Si – 0.35
S – 0.01
Cr – 0.30
Ni – 0.30

 

Mechanical Properties of 16Mo3 Sheets & Plates

Properties 16Mo3
Tensile Strength (Mpa) 440-590
Yield Strength (Mpa) 220-275
Elongation in 100-150 mm(%) 19
Elongation in 16 mm(%) 24
Max Thickness (mm) 250
Shear Modulus 79.3 GPa

 

16Mo3 Sheets & Plates – Equivalent Grades

STANDARD 16Mo3
WERKSTOFF NR. 1.5415
UNS –
JIS JIS G3115
EN EN10028
BS 1503-243B
GOST –

 

 

ASTM A204 Alloy Steel Plate 100mm Thickness 16Mo3 Molybdenum 0ASTM A204 Alloy Steel Plate 100mm Thickness 16Mo3 Molybdenum 1ASTM A204 Alloy Steel Plate 100mm Thickness 16Mo3 Molybdenum 2

Hot Tags: astm a204 alloy steel plate 100mm thickness 16mo3 molybdenum, China astm a204 alloy steel plate 100mm thickness 16mo3 molybdenum suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS409 Stainless Steel Welded Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry