Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 321/321h sheets and plates in China. If you're going to wholesale high quality stainless steel 321/321h sheets and plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 321/321H is Titanium stabilized stainless steel plate and sheet with good mechanical properties. These stainless steel plates and sheets offer excellent corrosion resistance and have excellent resistance to inter-granular corrosion after exposing it in the chromium carbide range of temperatures. They also have higher creep and stress rupture properties compare to other alloys. Stainless steel 321/321H plates also offer good low-temperature toughness and superior strength. These 321h plates also used in diluted organic acid at medium temperatures. They also offer some other features like high tensile strength, durability, precise design and so on.



Types ofThe SS 321/321H Sheets & Plates that we offer are Chequered Plate SS 321H Rolls, Cold Rolled Plates, 321/321H Coils, Strips, Foils, Shim Sheet, Perforated Sheet, Circle, Polished Plates, Hot Rolled Plates, Rings, and many more.
There are many industrial applications in which these stainless steel plates and sheets are utilized and offer excellent performance. Several applications of SS 321/321H Sheets & Plates are power generation plants, off-shore oil drilling refineries, gas processing industry, Specialty Chemicals, Pharmaceuticals, Pharmaceutical Equipment, Chemical Equipment, Heat Exchangers, Pulp and Paper Industry, Petrochemicals, and so on.
WE provide all the material test certificates in accordance with EN 20204/3.1B and some of them are Raw Materials Certificate, 100% Radiography Test Report, Third Party Inspection Report, and so on. We also did different material testing on these products to ensure the quality of these products before we dispatch them to our patrons.
321/321H STAINLESS STEEL SHEETS AND PLATES EQUIVALENT GRADES
| STANDARD | UNS | WNR. | JIS | EN |
|---|---|---|---|---|
| SS 321 | S32100 | 1.4541 | SUS 321 | X6CrNiTi18-10 |
| SS 321H | S32109 | 1.4878 | SUS 321H | X12CrNiTi18-9 |
Stainless Steel Sheets and Plates Specification : ASTM A240 / ASME SA240
Dimension Standard : JIS, AISI, ASTM, GB, DIN, EN, etc
Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc
Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc
Thickness : 0.3 mm to 120 mm
Form : Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) etc.
Surface Finishing : Hot rolled plate (HR), Cold rolled sheet (CR),2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, Chequered, embossed, hair line, sand blast, Brush, etching, SATIN (Met with Plastic Coated) etc.
CHEMICAL COMPOSITION OF STAINLESS STEEL 321/321H SHEETS AND PLATES
| % | Cr | Ni | C | Si | Mn | P | S | N | Ti | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| 321 | min:17.0 max:19.0 |
min: 9.0 max:12.0 |
max:0.08 | max:0.75 | max:2.0 | max:0.045 | max:0.03 | max:0.10 | min:5*(C+N) max:0.70 |
Balance |
| 321H | min:17.0 max:19.0 |
min: 9.0 max:12.0 |
min:0.04 max:0.10 |
min:18.0 max:20.0 |
max:2.0 | max:0.045 | max:0.03 | max:0.10 | min:5*(C+N) max:0.70 |
Balance |
MECHANICAL PROPERTIES OF STAINLESS STEEL 321/321H SHEETS AND PLATES
| Grade | Tensile Strength ksi (min.) |
Yield Strength 0.2% Offset ksi (min.) |
Elongation - % in 50 mm (min.) |
Hardness (Brinell) MAX |
|---|---|---|---|---|
| 321/321H | 75 | 30 | 40 | 217 |
Hot Tags: stainless steel 321/321h sheets and plates, China stainless steel 321/321h sheets and plates suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate