Stainless Steel 304H Steel Strip
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 304h steel strip in China. If you're going to wholesale high quality stainless steel 304h steel strip made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 304H Strip is a T-300 series stainless steel austenitic, which has a minimum of 18% chromium and 8% nickel with a maximum of 0.08% carbon. It is the standard "18/8 stainless" that is commonly found in pans and cooking tools. Stainless Steel 304H Strip is the most versatile and widely used alloy in the stainless steel family. It may be used for a wide variety of home and commercial applications and exhibits excellent corrosion resistance, has a high ease of fabrication, outstanding formability, and tremendous strength.

STAINLESS STEEL 304H STRIP CHEMICAL PROPERTIES:
| % | Cr | Ni | C | Si | Mn | P | S | N |
|---|---|---|---|---|---|---|---|---|
| 304H | min: 18.0 max:20.0 |
min: 8.0 max: 10.5 |
min: 0.04 max:0.10 |
0.75 max |
2.0 max |
0.45 max |
0.03 max |
0.10 max |
STAINLESS STEEL 304H STRIP MECHANICAL PROPERTIES:
| Grade | Tensile Strength ksi (min.) |
Yield Strength 0.2% Offset ksi (min.) |
Elongation - % in 50 mm (min.) |
Hardness (Brinell) MAX |
Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 304H | 75 | 30 | 40 | 201 | 92 |

The austenitic stainless steels are also considered to be the most weldable of the high-alloy steels and can be welded by all fusion and resistance welding processes. Due to its controlled carbon content of 0.04 to 0.10, Alloy 304H provides improved high temperature strength when exposed to temperatures above 800oF. Stainless Steel 304H Strip also has greater short term and long term creep strength than Alloy 304L at temperatures above 500oC and is more resistant to sensitization than Alloy 304L.
Hot Tags: stainless steel 304h steel strip, China stainless steel 304h steel strip suppliers, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates