Stainless 304 Steel Plate And Sheet
video

Stainless 304 Steel Plate And Sheet

304 is the most widely used grade of all the stainless steels. It is preferred for its good corrosion and thermal resistance, sufficient mechanical properties in normal environments, strength at tempratures below 700°C, good formability, good forgeability and excellent weldability.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 304 steel plate and sheet in China. If you're going to wholesale high quality stainless 304 steel plate and sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

304 is the most widely used grade of all the stainless steels. It is preferred for its good corrosion and thermal resistance, sufficient mechanical properties in normal environments, strength at tempratures below 700°C, good formability, good forgeability and excellent weldability.

4 222

Machinability is average with the right tools. For detailed processes 303 grade must be preferred. Heat resistance is up to 700°C, other heat resistant grades must be preferred for higher degrees. 304 grade is in austenitic family and it is available in all of the stainless steel forms and shapes. It is the optimal grade for standard applications.With its availability, and optimal performance in standard conditions, 304 grade has a well deserved fame in Austenitic family.

Grade
(AISI)

C

Mn

Si

P

S

Cr

Mo

Ni

N

304

min.

max.

-

0.08

-

2.0

-

0.75

-

0.045

-

0.030

18.0

20.0

-

8.0

10.5

-

0.10

304L

min.

max.

-

0.03

-

2.0

-

0.75

-

0.045

-

0.030

18.0

20.0

-

8.0

10.5

-

0.10

4 376

When you consider the aesthetical apperance, polishability, cold forming capability, good mechanical properties, good corrosion resistance and excellent weldability, 304 grade is a natural leader in Austenitic Family with its price / performance ratio.

Hot Tags: stainless 304 steel plate and sheet, China stainless 304 steel plate and sheet suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry