RINA FH36 Shipbuilding Steel Plate, Hot Rolled Steel Plate 2mm - 200mm Thickness
video

RINA FH36 Shipbuilding Steel Plate, Hot Rolled Steel Plate 2mm - 200mm Thickness

FH36 is a high strength ship steel grade, in -60 charpy V impact and normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of rina fh36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness in China. If you're going to wholesale high quality rina fh36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

RINA FH36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness

Description

Name: Ship Steel Plate Material: A D E F Grade
Length: 6-11m Width: 1500-2500mm
Thickness: 5-250mm Type: Hot Rolled
High Light:

shipping plate

,

marine steel plate

RINA FH36 shipbuilding steel plate, F36 Ship steel, hot rolled steel plate for ship structure

 

supply steel grade RI/A36, RI/D36, RI/EH36, RI/F36, RI/A32, RI/D32, RI/E32, RI/F32, RI/A, RI/B, RI/D,RI/E. RI/A40, RI/D40, RI/E40, RI/F40.

 

FH36 is a high strength ship steel grade, in -60 charpy V impact and normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.

Description

Name

ship building steel plate AH32,AH36,AH40

Specification

as your requirement

Thickness

2mm~200mm

Width

500mm~3000mm

Length

2000mm-18000mm(as your requirements)

manufacturing technique

Hot rolled

Surface treatment

coated

Standards

ASTM

application

ship building steel plate

Packaging

Standard exporting packing or as client's requirement

Certificate

Quality Testing Report /ISO9001:2008/Mill test Certificate

The above are the general items, for the special types,

we can also meet your needs

 

About FH36 detail information,please check technical date in following.

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

FH36

0.160

0.10-0.5

0.9-1.6

0.025

0.025

0.05-0.10

0.015

0.200

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.350

0.080

0.02-0.05

0.080

0.020

0.012

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

FH36

8mm-50mm

Min 355Mpa

490-620Mpa

21%

-60

34J

51mm-70mm

Min 355Mpa

490-620Mpa

21%

-60

NA

71mm-100mm

Min 355Mpa

490-620Mpa

21%

-60

NA

The min impact energy is longitudinal energy

 

Our mill FH36 always be exported to Singapore and Thailand shipyard for shipbuilding.

To get our competitive quotation, please feel free to contact us.

 

RINA FH36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness 0RINA FH36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness 1

Hot Tags: rina fh36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness, China rina fh36 shipbuilding steel plate, hot rolled steel plate 2mm - 200mm thickness suppliers, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, Corrugated SS Roof Sheet, 400 2 4360 Alloy Pipe, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry