Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 2.4360 alloy sheet in China. If you're going to wholesale high quality monel 2.4360 alloy sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel 2.4360 Alloy Sheet
Product Introduction
Monel Alloy 400 is a nickel-copper (about 67% Ni – 23% Cu) solid solution strengthened alloy. The alloy is characterized by moderate strength, good weldability, good general corrosion resistance and toughness. It is useful at temperatures up to 1000°F (538°C). Alloy 400 has excellent resistance to rapidly flowing brackish or seawater where cavitation and erosion resistance is necessary. It is particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated. Alloy 400 is slightly magnetic at room temperature.
Chemical Composition
| Trade Name |
ASTM/AISI Alloy type |
UNS | %Cu | %Fe | %Mn | %Si | %Ni |
| Monel 400 | B 127, B 164 | N04400 | 28–34 | 2.5 max | 2.0 max | 0.5 max | 63 min |
Hot Tags: monel 2.4360 alloy sheet, China monel 2.4360 alloy sheet suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate, 400 2 4360 Alloy Pipe