Maraging 250 is an age hardenable iron-nickel steel alloy melted as VIM + VAR with ultra high strength and toughness. This alloy is easily machinable in the annealed condition prior to final heat treatment. This grade has improved fracture toughness from Maraging 300 but slightly less strength. The unique properties makes it suitable for many critical aerospace applications
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of maraging 250 alloy ss plate in China. If you're going to wholesale high quality maraging 250 alloy ss plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Maraging 250 is an age hardenable iron-nickel steel alloy melted as VIM + VAR with ultra high strength and toughness. This alloy is easily machinable in the annealed condition prior to final heat treatment. This grade has improved fracture toughness from Maraging 300 but slightly less strength. The unique properties makes it suitable for many critical aerospace applications

 

Common Trade Names:

Alloy 250 , UNS K92890 , Vascomax C250 , Maraging 250 , Maraging C250 , X1NiCoMo18-8-5 , W.Nr 1.6359

Specifications:

AMS 6512, BS S162, DTD 5212, G110, Mil-S-46850D

Characteristic:

Excellent Mechanical Properties

high yield and ultimate tensile strengths

high toughness, ductility and impact strengths

high fatigue strength

high compressive strength

hardness and wear resistance sufficient for many tooling applications

Excellent Workability

high resistance to crack propagation

readily formed – cold, warm, hot (w/o in process anneals)

good weldability w/o preheating or post heating

excellent polishability

Advantages During Application

low coefficient of expansion minimizes heat checking

pitting and corrosion resistance superior to common tool steel

good repair weldability

excellent mechanical properties have led to longer tool life

easily reworked and retreated for secondary tool life

Maraging 250 Chemical Composition

% C Si Mn P S Al B Ca Co Cr Mo Ni Ti Zr Cu Fe
Min – – – – – 0.05 – – 7 – 4.6 17 0.3 – – Bal
Max 0.03 0.1 0.1 0.01 0.15 0.15 0.005 0.05 8.5 0.5 5.2 19 0.5 0.02 0.05  

Maraging 250 Physical Properties

Density Modulus of Elasticity Average Co of Thermal Expansion
8.0 g/cm 27.0 x 10-6 psi 5.6 x 10-6 in/in/°F

Maraging 250 Heat Treatment / Aging:

Maraging alloys are essentially carbon-free, a protective atmosphere is not required during annealing or aging. Material is supplied in the solution annealed condition with a hardness of 30/35 Rc. Typical heat treat time/temperature are listed below. Large cross sections should be aged for longer periods.

NOTE: A modified aging cycle is suggested for die casting applications for increased die life. The following thermal treatments have been used to obtain desirable characteristics for die casters. Following the rough machining of the die, anneal at 1500-1525 ºF for 1 hour per inch of thickness is typical. After finish machining, an aging heat treatment of 980-1000 ºF for 6 hours is typical.

Temperature Time Resulting Hardness
900/925 °F 6 hrs 48/52 Rc

Maraging 250 Available Shape

Maraging 250 Size Range

Bars & Rods & Foring Ring /Flanges

Sheet & Plate

Strip & Coil

Welding Wire &Spring wire

Seamless Tube & Welded Pipe

 

 

 

product-720-720product-720-720product-720-720product-720-720

Maraging 250 ApplicationsI

Aircraft assemblies

Mortar tubes

Extrusion dies

Rocket motor cases

Pressure vessels

 

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: maraging 250 alloy ss plate, China maraging 250 alloy ss plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS431 Stainless Steel Plate, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry