Hot Rolled SAE 1045 4-120mm CK 45 Carben Steel Plates For General Machinery Parts
video

Hot Rolled SAE 1045 4-120mm CK 45 Carben Steel Plates For General Machinery Parts

Hot rolled SAE 1045 4-120mm CK 45 carben steel plates for general machinery parts Description Name: Carben Steel Plate Technique: Hot Rolled Width: 1000-2500mm Length: 6-13m High Light: low carbon steel plate , carbon steel sheet SAE 1045 steel plate ,SAE 1045 carbon steel plate
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hot rolled sae 1045 4-120mm ck 45 carben steel plates for general machinery parts in China. If you're going to wholesale high quality hot rolled sae 1045 4-120mm ck 45 carben steel plates for general machinery parts made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hot rolled SAE 1045 4-120mm CK 45 carben steel plates for general machinery parts

Description

Name: Carben Steel Plate Technique: Hot Rolled
Width: 1000-2500mm Length: 6-13m
High Light:

low carbon steel plate

,

carbon steel sheet

SAE 1045 steel plate ,SAE 1045 carbon steel plate

 

Sizes

Thickness: 6-800mm

Width:200-2000mm

Length:2000-6000mm

 

Application

 

- Carbon steel AISI 1045 Used for making die-board,general machinery parts.

 

- Component parts for vehicles, shafts, bushings, crankshafts, connecting rods and parts for the machine building industry and steel for axes, knives, hammers etc.

 

 

Equivalent Grade

GB

DIN

NF

SS

JIS

BS

AISI

ISO

45#

1.0503

C45

1650

S45C

IC45/080A47

1045

C45E4

 

 

 

 

Chemical Analysis

NO.

C

Mn

Si

Cr

Cu

Ni

P

S

Aisi 1045

0.43~0.50

0.6~0.9

0.10~0.60

 

 

 

≤0.40

≤ 0.50

DIN1.0503

0.42~0.48

0.6~0.9

0.15~0.35

≤0.15

≤0.3

≤0.2

 

 

JIS S45C

0.42~0.50

0.5~0.8

≤0.40

≤0.40

 

≤ 0.4

   

GB45

0.42~0.50

0.5~0.8

0.17~0.37

≤0.25

≤0.25

≤0.3

≤0.035 ≤0.035

 

Mechanical properties

Annealing

Forging

Tempering and Hardening

Normalization

Subcritical annealing:

650~700

Isothermal annealing:

820~860

1100~850

Tempering: 550~660

Hardening : 820~860 water

840~880

 

Heat Treatment

Soft annealing: heat to 550-650°C, cool slowly.

Hardness after annealing: Max. 269HB

Hardening: 820 - 870 °C

Normalizing temperature: 840-870°C

Hot rolled SAE 1045 4-120mm  CK 45 carben steel plates for general machinery parts 0Hot rolled SAE 1045 4-120mm  CK 45 carben steel plates for general machinery parts 1

 

Hot Tags: hot rolled sae 1045 4-120mm ck 45 carben steel plates for general machinery parts, China hot rolled sae 1045 4-120mm ck 45 carben steel plates for general machinery parts suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates

Send Inquiry

whatsapp

Phone

E-mail

Inquiry