Ferrite Stainless Steel 316L Round Plate
video

Ferrite Stainless Steel 316L Round Plate

EN 1.4404 material (stainless steel X2CrNiMo17-12-2) is a low-carbon version of 1.4401 (X5CrNiMo17-12-2), the maximum carbon content is only 0.03%, while 1.4401 is 0.07% maximum, so the weldability and corrosion resistance of 1.4404 stainless steel is better than 1.4401. The chemical composition of material 1.4404 and 1.4401 contain molybdenum (Mo), while EN 1.4301 (X5CrNi18-10) and 1.4307 (X2CrNi18-9) do not. Molybdenum improves the heat resistance of steel and resists pitting and crevice corrosion in environments containing chlorides or other halides.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ferrite stainless steel 316l round plate in China. If you're going to wholesale high quality ferrite stainless steel 316l round plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

EN 1.4404 material (stainless steel X2CrNiMo17-12-2) is a low-carbon version of 1.4401 (X5CrNiMo17-12-2), the maximum carbon content is only 0.03%, while 1.4401 is 0.07% maximum, so the weldability and corrosion resistance of 1.4404 stainless steel is better than 1.4401. The chemical composition of material 1.4404 and 1.4401 contain molybdenum (Mo), while EN 1.4301 (X5CrNi18-10) and 1.4307 (X2CrNi18-9) do not. Molybdenum improves the heat resistance of steel and resists pitting and crevice corrosion in environments containing chlorides or other halides.1.4404 material is normally firstly processed into many intermediate products such as square steel, round steel, sheet steel, steel strip, steel rods and other forms of steel bars, etc., and then processed into finished products such as pipe fittings, angle steel, stainless steel wire mesh, decorative fabrics, filter element, filter cartridges, flanges, valves, elbows, watch straps, etc. are widely used in aerospace, petrochemical, architectural decoration, and daily necessities industries.

Compared to stainless steel 1.4401, it can be easily welded using a variety of conventional welding methods due to its extremely low carbon content and does not require annealing after welding.

  Mechanical properties (solution annealed)
Standard Steel Grade (Steel Number) Diameter (d) or Thickness (t) in mm Hardness (HB) 0.2% yield strength (N/mm2) 1% yield strength (N/mm2) Tensile strength (N/mm2) Elongation (%) Impact energy (J)
EN 10088-3 X2CrNiMo17-12-2 (1.4404) d≤160 ≤ 215 ≥ 200 ≥ 235 500-700 40 (Longitudinal) ≥ 100 (Longitudinal)
160<t≤250 30 (Transverse) ≥ 60 (Transverse)
    Mechanical properties for bright bars (solution annealed)
Standard Steel Grade (Steel Number) Diameter (d) or Thickness (t) in mm 0.2% yield strength (N/mm2) ≥ Tensile strength (N/mm2) Elongation (%) ≥ Impact energy (J) ≥
EN 10088-3 X2CrNiMo17-12-2 (1.4404) d≤10 400 600-930 25 –
10<t≤16 400 580-930 25 –
16<t≤40 190 500-830 30 100
40<t≤63 190 500-830 30 100
63<t≤160 190 500-700 40 100
160<t≤250 190 500-700 30 (Transverse) 60 (Transverse)

product-225-225product-225-225product-225-225product-369-360product-317-313product-317-313

FAQ

Q: Can provide OEM/ODM service?

A: Yes. Please feel free to contact us for more details discuss.

Q: How is your Payment Term?

A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Hot Tags: ferrite stainless steel 316l round plate, China ferrite stainless steel 316l round plate suppliers, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, SS431 Stainless Steel Plate, 400 2 4360 Alloy Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry