Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients’ requirements Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish Form : Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc Surface : Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline Condition : Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c276 round rod hastelloy astm b574 uns n10276 annealed straight ends bar in China. If you're going to wholesale high quality c276 round rod hastelloy astm b574 uns n10276 annealed straight ends bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

C276 Round Rod Hastelloy ASTM B574 UNS N10276 Annealed Straight Ends Bar

Description

Grade: Nickel Base Alloy,Hastelloy C276 Application: Industry,construction,used In Chemical,spun
Type: Nickel Bar Ni (min): Balance
Surface: Polished,Black Or Bright Standard: ASTM,DIN,EN,AISI
Material: No 10276 Size: According To Client's Requirements,as Required
High Light:

Annealed Straight Ends Bar

,

C276 Hastelloy Round Rod

,

ASTM B574 Hastelloy Round Rod

Stock Size Range and Specifications For ASTM B574 Hastelloy C276 Round Bar

Specification : EN, DIN, JIS, ASTM, BS, ASME, AISI

Standard Specification : ASTM B574 / ASME SB574

Size : 15NB to 150NB IN

Diameter : 3.17mm to 350mm diameter

Length : 100 mm to 3000 mm Long & Above

Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements

Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Form : Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc

Surface : Hot Rolled Pickled or Sand Blasting Finished, Cold Drawn, Bright, Polished, Hairline

Condition : Cold Drawnd Pulished Cold Drawn Centreless Ground & Polished

 

Chemical Composition of Hastelloy C276 Round Bars
Grade C Mn Si S Co Ni Cr Fe Mo P
C276 0.010 max 1.00 max 0.08 max 0.03 max 2.50 max 50.99 min* 14.50 – 16.50 4.00 – 7.00 15.00 – 17.00 0.04 max

 

Mechanical Properties of Hastelloy C276 / N10276 / 2.4819 Round Bars
Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C276 8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52,000 , MPa – 355 40 %

 

Markings On The Hastelloy C276 Round Bar

The full identification of the bars should be continuously marked down its whole length, including :

Rating Designation

Material Designation

"WP" in grade symbol

Grade

Schedule number or nominal wall thickness

Heat Code

Manufacturer's Name or Symbol

 

ASTM B574 Hastelloy C276 Bars Application Industries

Petrochemical Industry

Chemical Industry

Oil and Gas Industry

Pulp & Paper Indusry

Power Plant Industry

Food Processing Industry

Pharmaceuticals Industry

Energy Industry

Aerospace Industry

C276 Round Rod Hastelloy ASTM B574 UNS N10276 Annealed Straight Ends Bar 0C276 Round Rod Hastelloy ASTM B574 UNS N10276 Annealed Straight Ends Bar 1C276 Round Rod Hastelloy ASTM B574 UNS N10276 Annealed Straight Ends Bar 2

Hot Tags: c276 round rod hastelloy astm b574 uns n10276 annealed straight ends bar, China c276 round rod hastelloy astm b574 uns n10276 annealed straight ends bar suppliers, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry