Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a516 gr 70 n boiler steel plate for pressure vessel in China. If you're going to wholesale high quality astm a516 gr 70 n boiler steel plate for pressure vessel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASTM A516 GR 70 N Boiler Steel Plate For Pressure Vessel
Description
| Width: | 600-2500mm | Application: | Boiler Plate |
|---|---|---|---|
| Technique: | Hot Rolled | Type: | Steel Plate |
| Standard: | ASTM ASME | Length: | 1000-12000mm |
| Special Use: | Pressure Vessel Boiler | Thickness: | 1mm-120mm |
| Surface: | Black Painted | Product Name: | Boiler Quality Pressure Vessel Steel Plate |
| High Light: |
ASTM A516 Boiler Steel Plate,GR 70 N Boiler Steel Plate,Pressure Vessel Boiler Plate Steel |
||
ASTM A516 GR 70 N 100%-ULTRASON TEST NO BENDING NO OXIDATION Boiler Steel Plate For Pressure Vessel
| Product Name | Pressure Vessel Carbon Steel Plate |
| Standard | ASTM, AISI, GB, JIS, DIN, BS,En |
| Grade | SA516 GR70, SS400,S355JR ,A53,A36,SM400A,St37-2,SA283Gr,S235JR,S235J0,S235J2 Q245R,Q345R,Q370R,15CrMoR,18MnMoNbR,13MnNiMoR 12Cr1MoVR,12Cr2Mo1R,14CrMoR 16MnDR,09MnNiDR,15MnNiDR 07MnCrMoVR,07MnNiCrMoVDR/12MnNiVR SPV235,SPV315,SPV355,SPV410,SPV490 HI,HII,10CrMo910,15Mo3,13CrMo44,19Mn6 (s)A387M(GR11,12,22), (s)A537M(GL1,CL2) (s)A662M(GrA,B,C), (s)A302M(GraA,B,C,D), (s)A737M(Gr.B,C) P235GH,P265GH,P395GH,P355GH,16Mo3 |
| Thickness | 3-500mm or customized as required |
| Width | 600-3000mm or customized as required |
| Length | 4-12m or customized as required |
| Surface Treatment | Clean, Finishing, Blasting and Painting |
| Coil Weight | 3-5 Tons or customized as required |
| Processing Service | Bending, Welding, Decoiling, Cutting, Punching |
| Delivery States | Hot-rolled, controlled rolling, normalizing, annealing, tempering, quenching, N+T, Q+T, and other delivery states as your request |
| Sample | Sample Freely |
| Characteristic | Good corrosion resistance, high strength, good weldability, safe and reliable |
| OEM Service | Perforated, Cutting special size, Doing flatness, Surface treatment, etc |
| Certifications | API,ISO,SGS,BV,CE etc |
| Transport Package | Export Standard Package or as Request |
| Payment terms | T/T,L/C |
| Loading Port | Tianjin/Qingdao/Shanghai Port |
| Application | Mainly used in the manufacture of various pressure vessels, boilers, storage tanks, heat exchangers, separators, spherical tanks, hydrogenation reactors, oxidation reactors, adsorption towers, absorption towers, evaporators, hydrocracking reactors and other chemical equipment and Containers, as well as petroleum, chemical, electric power, boiler and other industries. In addition, pressure vessel plates can also be used to manufacture important engineering structural parts such as ships, bridges, and building structures. |
| Export market | Europe, Africa, Central Asia, Southeast Asia, Middle East, South America, North America, etc |
Detailed Photos


Grade of our steel plate (ASTM Grade as Guide)
| Structural Steel | A283,A36,ABS Grade A, Grade B, Grade ADH36, Grade DH36, and Grade EH36,A514 T-1,A572 GR 50: |
| HSLA Structural Steel | A588,A656 GR80,A690 |
| Pressure vessel Steel | A285 GR C, A515 GR 70,A516 GR 70,SA537 |
| Abrasion resistant steel | AR360,AR400,AR450,AR500 |
| Alloy Steel | 5130,5140,5150,4130,4140 |
The company mainly engaged in thick plate, round steel, steel pipe NC cutting processing business, distribution as one. Main business: Shagang, cultivation, baosteel, yingkou, masteel, xingcheng, WuGang large steel mills such as alloy plate (40 cr / 35 crmo / 42 crmo / 65 mn) container board, boiler (Q245R/Q345R ASME SA516GR70), plate (Q235A/B), low alloy (Q345B/Q345C/Q345D/Q345E/Q690D) , carbon plate (45#), wear-resisting plate (NM360/NM400/NM450/NM500) Boiler Plate and other specifications, all kinds of material material specifications for the thickness of 1mm-400mm, can also be processed according to customer drawings. With many years of cutting experience, the company integrates the cutting characteristics of high precision of finished products, neat incision and processing allowance less than one, which is recognized by customers.
With the continuous expansion of the company's scale and the accumulation of customer resources, the company has added 6 large CNC flame and plasma cutting equipment, a number of small CNC equipment, fully meet the requirements of customers on quantity and quality. And in order to ensure that the material let the user rest assured, special material zero cutting can be in accordance with customer requirements of the whole video operation.
Our Service




We can provide variety kinds of service for our Products, inlcude cutting, bending.etc
Our Cutting Service
| Service Name | Cutting (Laser Cutting, Waterjet Cutting) |
| Thickness | 3.0 - 150.0mm |
| Length | Within 12000mm |
| Platform Size | 2500*12000mm |
| Tolerance | within 2mm |
Equipment List
| Laser Cutting | 2 Sets Cutting range: within 30mm |
| Waterjet Cutting | 1 Set Cutting range within 100mm |
| Plasma Cutting | 3 Set Cutting range : within 150mm |
| Sawing Machina | 1 Set Cutting range: above 50mm |
| Bending | 1 Set thickness range within 20mm |
Applications for Steel Sheet & Steel Plate
Durable, adaptable, and easy to work with, steel sheet and plate can be used to create a huge variety of products and structures. Common applications for steel plate and sheet include:
Building & construction
Automotive & transportation
Shipping containers
Roofing
Appliances
Heavy equipment
Hot Tags: astm a516 gr 70 n boiler steel plate for pressure vessel, China astm a516 gr 70 n boiler steel plate for pressure vessel suppliers, SS409 Stainless Steel Welded Pipe, SS431 Stainless Steel Plate, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, 400 2 4360 Alloy Pipe
You Might Also Like
Send Inquiry