Astm A514 Carbon Steel Plate 6.0*2000*8000mm Quenched And Tempered
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a514 carbon steel plate 6.0*2000*8000mm quenched and tempered in China. If you're going to wholesale high quality astm a514 carbon steel plate 6.0*2000*8000mm quenched and tempered made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Astm A514 Carbon Steel Plate 6.0*2000*8000mm Quenched And Tempered
Description
| Thickness: | 3-150mm | Surface: | NO.1 |
|---|---|---|---|
| Width: | 1000-2000mm | Length: | 2000-12000mm |
| Grade: | ASTM A514 | Application: | Boiler Plate,Ship Plate |
| Technique: | Hot Rolled | Standard: | ASTM,AISI,JIS,DIN |
| Special Use: | Pressure Vessel Boiler | ||
| High Light: |
astm a514 carbon steel plate,quenched and tempered carbon steel plate,6mm thick carbon steel sheet |
||
A514 STEEL PLATE
ASTM A514 is most commonly used as structural steel in cranes and large heavy-load machines. Leeco® Steel stocks ample inventory of A514.
WHAT IS A514/T-1 STEEL PLATE?
ASTM A514 steel plate, also known as T-1 steel plate, is a popular grade of quenched and tempered (Q&T) steel that offers high strength, weldability and machinability. Due to these properties, A514 is typically used in applications where wear resistance and the ability to withstand high impact are important.
A514 is heat-treated through quenching and tempering, a two-step heat treatment process that alters the grain structure of the material to increase strength, hardness and toughness.
A514/T-1 plate is available in eight grades: Grade B, Grade S, Grade H, Grade Q, Grade E, Grade F, Grade A and Grade P. The mechanical properties of these grades depend on thickness, but chemical properties may vary between grades.
Overview:
Commonly used as structural steel in cranes or large heavy-load machines, A514 offers high strength with weldable, machinable properties.
Also referred to as T-1 steel.
Quenched and tempered for increased strength.
Available in eight grades: B, S, H, Q, E, F, A and P.
Available in heavy plate thicknesses (3-inches or greater).
Suitable in lower temperatures. Charpy impact test results for specific climates available.
Select grades are available to purchase online v
Available Sizes
Leeco Steel stocks the following standard sizes, but other sizes may be available for special orders.
| GRADE | THICKNESS | WIDTH | LENGTH |
| GRADE B | 3/16" – 1 1/4" | 48" – 120" | UP TO 480" |
| GRADE S | 3/16" – 2 1/2" | 48" – 120" | UP TO 480" |
| GRADE H | 3/16" – 2" | 48" – 120" | UP TO 480" |
| GRADE Q | 3/16" – 8" | 48" – 120" | UP TO 480" |
| GRADE E | 3/16" – 6" | 48" – 120" | UP TO 480" |
| GRADE F | 3/16" – 2 1/2" | 48" – 120" | UP TO 480" |
| GRADE A | INQUIRE | INQUIRE | INQUIRE |
| GRADE P | INQUIRE | INQUIRE | INQUIRE |
Benefits of A514/T-1 Steel Plate
A514 steel plate's chemical composition and heat treatment give the material greater toughness and strength compared to non-heat-treated carbon steel plate. These properties enable the material to withstand high levels of wear and make it a durable, long-lasting material.
The durability of A514 plate means it will need to be replaced less frequently than other, less durable materials, which can help save material costs in the long run.
A514/T-1 Equivalent Grades
While A514 steel is governed by ASTM code, which is widely accepted across the globe, some specific projects may require materials that are certified to meet other standards. For projects requiring EN standard materials, EN S700 or EN690 may be possible alternatives to A514, depending on project requirements.
Other Q&T steel plate grades have similar properties to A514 plate and may be suitable for use high wear and stress applications.
Applications & Industries
A514 steel plate is typically used for applications that require high resistance to wear and great strength without sacrificing weldability and machinability, such as construction equipment – like cranes – and use in industrial manufacturing, including heavy-load machines.
MATERIAL PROPERTIES
The following material properties are ASTM specifications and will be confirmed on the Mill Test Report.
| GRADE | YIELD POINT (KSI) | TENSILE STRENGTH (KSI) | MIN. 8" ELONGATION % |
| 3/4" OR LESS THICKNESS | 100 | 110-130 | 18 |
| GREATER THAN 3/4" TO 2.5" THICKNESS | 100 | 110-130 | 18 |
| GREATER THAN 2.5" TO 6" THICKNESS | 90 | 100-130 | 16 |



Hot Tags: astm a514 carbon steel plate 6.0*2000*8000mm quenched and tempered, China astm a514 carbon steel plate 6.0*2000*8000mm quenched and tempered suppliers, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe, SS410 Stainless Steel Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, ASTM A240 Grade 431 10mm Stainless Steel Plate