1.4567 1.4565 Medium And Thick Plate
video

1.4567 1.4565 Medium And Thick Plate

Applications: • Automotive industry • Chemical industry • Food and beverage industry • Decorative items and kitchen utensils • Electronic equipment • Ship building.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4567 1.4565 medium and thick plate in China. If you're going to wholesale high quality 1.4567 1.4565 medium and thick plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Products Description

1.4567 1.4565 Medium and Thick Plate

Austenitic stainless steel 18/8 with copper. This alloying addition makes it ductile for cold-heading and thread rolling applications, for example corrosion-resistant fasteners. Other applications are heat exchangers, coolers, tanks and pumps in paper and food processing plants, ship components and electronics. The steel has very good machinability and is very ductile, even in sub-zero temperature. It is not magnetic, nor it becomes magnetic after cold working.

Products Properties

 

Chemical composition of stainless steel 1.4567

C

Mn

P

S

N

Cr

Cu

Mo

Ni

Ti

Si

≤ 0,04

≤ 2,00

≤ 0,045

≤ 0,03

≤ 0,10

17,0 - 19,0

3,0 - 4,0

-

8,5 - 10,5

-

≤ 1,00

Mass fraction in % according to DIN EN 10088-3

Mechanical Properties

Type Tensile Strength, ksi (MPa), Max Elongation in 10 in. (254 mm), Min Diameter, d, mm Diameter, d, in Condition
304L 145 (1,000) 30 0.05-0.13 0.002-0.005 Annealed or bright annealed
135 (930) 30 0.13<d≤0.23 0.005<d≤0.009
130 (900) 35 0.23<d≤0.38 0.009<d≤0.015
125 (860) 40 0.38<d≤0.51 0.015<d≤0.020
120 (830) 40 0.51<d≤0.64 0.020<d≤0.025
115 (790) 40 0.64<d≤0.89 0.025<d≤0.035
110 (760) 45 0.89<d≤1.09 0.035<d≤0.043
105 (720) 45 >1.09 >0.043
120 (830)-150 (1030) 15 0.76-3.18 0.03-0.125 Cold drawn
110 (760)- 140 (970) 15 >3.18 >0.125

1.4567 1.4565 Medium and Thick Plate

medium-thick steel plate

The austenitic material 1.4567, which is comparable to both AISI 302 HQ and AISI 304 Cu, is a chromium-nickel stainless steel. It differs from the otherwise similar material 1.4301 / AISI 304 in its copper content of 3-4 %, which contributes to the fact that stainless steel 1.4567 is ideally suited for cold forming. It can also be used at low temperatures.

The material 1.4567 has good forging properties and good corrosion resistance (but not to salt water). It is used, among other things, in the automotive industry and for the production of screws.

Alloy 24 (1.4565) is an austenitic stainless steel distinguished by its excellent corrosion resistance and high strength. In fact, due to its high pitting index – known as pitting resistance equivalent number (PREN) – Alloy 24 belongs to the super austenitic stainless-steel group. This is a class of materials derived from further developing austenitic stainless steels to fill the gap between standard grades of stainless steels and nickel-based alloys.

Customer Case

 

Stainless Steel Medium Thickness Plate

FAQ

 

Q: Do you provide customized product services?
A:Yes, we can produce according to your specifications and drawings.
Q: Can I visit your factory?
A:Customers from all over the world are welcome to visit our factory.
Q: Can you assist me in importing steel for the first time?
A:Yes, we have freight forwarders who will work with you to arrange shipment.
Q:What is your delivery time?
A:Within 7 working days after receiving the balance payment.

Q:How do you make our business long-term and good relationship?
A:We keep good quality and competitive price to ensure our customers benefit ; We respect every customer as our friend and we sincerely do business and make friends with them. No matter where they come from.

Hot Tags: 1.4567 1.4565 medium and thick plate, China 1.4567 1.4565 medium and thick plate suppliers, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate