Astm A240 Gr Tp347 Tp347h Stainless Steel Plates
video

Astm A240 Gr Tp347 Tp347h Stainless Steel Plates

Alloy 347 is a stabilized, austenitic, chromium steel containing columbium which allows for the elimination of carbide precipitation, and, consequently, intergranualr corrosion. Alloy 347 is stabilized by the additions of chromium and tantalum and offers higher creep and stress rupture properties than alloy 304 and 304L which may also be used for exposures where sensitization and intergranualr corrosion are of concern. The addition of columbium also allows Alloy 347 to have excellent corrosion resistance, even superior to that of alloy 321. 347H is the higher carbon composition form of Alloy 347 and demonstrates improved high temperature and creep properties.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a240 gr tp347 tp347h stainless steel plates in China. If you're going to wholesale high quality astm a240 gr tp347 tp347h stainless steel plates made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 347 is a stabilized, austenitic, chromium steel containing columbium which allows for the elimination of carbide precipitation, and, consequently, intergranualr corrosion. Alloy 347 is stabilized by the additions of chromium and tantalum and offers higher creep and stress rupture properties than alloy 304 and 304L which may also be used for exposures where sensitization and intergranualr corrosion are of concern. The addition of columbium also allows Alloy 347 to have excellent corrosion resistance, even superior to that of alloy 321. 347H is the higher carbon composition form of Alloy 347 and demonstrates improved high temperature and creep properties.

Alloy 347 is frequently used for the fabrication of equipment, which must be placed in service under severe corrosive conditions, and is also common to the petroleum refining industries. Applications that consistently used Alloy 347 include:

High temperature chemical processes

Heat exchanger tubes

High temperature steam service

High pressure steam pipes

Radiant superheaters

Boiler tubes

Heavy duty exhaust systems

General refinery piping

Corrosion Resistance:

Offers similar resistance to general, overall corrosion as Alloy 304

Used for applications where alloys such as Alloy 304 are vulnerable to intergranualr corrosion

Generally used for heavy welded equipment which cannot be annealed and for equipment which is operated between 800 to 150°F (427 TO 816°C)

Alloy 347 is preferred over Alloy 321 for aqueous and other low temperature environments

Primarily used in high temperature environments where resistance to sensitization is necessary, in turn preventing intergranualr corrosion at lower levels

Susceptible to stress corrosion cracking

Exhibits oxidation resistance similar to all other 18-8 austenitic stainless steels

product-317-313product-600-450product-818-614product-800-800

 

FAQ

Q: Can provide OEM/ODM service?

A: Yes. Please feel free to contact us for more details discuss.

Q: How is your Payment Term?

A: Our usual payment methods are T/T, L/C, D/A, D/P, Western Union, Money Gram, payment methods can be negotiated and customized with customers.

Q: Can I get samples before order ?

A: Yes, of course.We can produce by your samples or technical drawings ;

Q: Can I go to your factory to visit?

A: Of course, we welcome customers from all over the world to visit our factory ;

Q:What are the shipping ports?

A:Under normal circumstances, we ship from Shanghai, Tianjin, Qingdao, Ningbo ports, you can choose other ports according to your needs.

Hot Tags: astm a240 gr tp347 tp347h stainless steel plates, China astm a240 gr tp347 tp347h stainless steel plates suppliers, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet, ASTM A240 Grade 431 10mm Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, SS431 Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates

Send Inquiry

whatsapp

Phone

E-mail

Inquiry