Alloy 410 Stainless Steel Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 410 stainless steel plate in China. If you're going to wholesale high quality alloy 410 stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Alloy 410 stainless steel plate is the general purpose 12% chromium martensitic stainless steel that can be heat treated to obtain a wide range of mechanical properties. 410 stainless steel plate possesses high strength and hardness coupled with good corrosion resistance. Alloy 410 stainless steel plate is ductile and can be formed. It is magnetic in all conditions.

| Property | Value |
|---|---|
| Density | 0.28 lbs/in³ (7.74 g/cm³) |
| Specific Heat | 0.11 BTU/lb-°F (32 – 212°F) / 0.46 J/kg-°K (0 – 100°C) |
| Modulus of Elasticity | 29.0 x 10⁶ psi (200 GPa) |
| Thermal Conductivity | 14.4 BTU/hr/ft²/ft/°F (24.9 W/m-°K) at 200°F (100°C) |
| Melting Range | 2700 – 2790°F (1480 – 1530°C) |
| Electrical Resistivity | 22.50 Microhm-cm at 68°C / 57 Microhm-cm at 20°C |
Alloy 410 (UNS S41000) is a 12% chromium martensitic stainless steel plate that can be heat treated to obtain a wide range of mechanical properties. The alloy has good corrosion resistance along with high strength and hardness. In the annealed condition, 410 stainless steel plate is ductile and may be formed. It remains magnetic in both the annealed and heat treated conditions.
Hot Tags: alloy 410 stainless steel plate, China alloy 410 stainless steel plate suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate, SS431 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet
You Might Also Like
Send Inquiry