Alloy Uns N06002 Hastelloy X Plate 30mm Thickness

Alloy Uns N06002 Hastelloy X Plate 30mm Thickness

Alloy X materials can be cold rolled to various tempers. It cannot be hardened through heat treating. It is easily fabricated. Alloy X maintains excellent corrosion resistance. It is readily formed by cold-working. Machining Alloy X nickel
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy uns n06002 hastelloy x plate 30mm thickness in China. If you're going to wholesale high quality alloy uns n06002 hastelloy x plate 30mm thickness made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy Uns N06002 Hastelloy X Plate 30mm Thickness

Description

Grade: Nickel Base Alloy Hastelloy X Type: Nickel Plate
Ni (min): Balance Standard: ASTM,DIN,EN,AISI
Material: Hastelloy X Thickness: 1mm~30mm
Package: Wooden Boxes Package
High Light:

uns n06002 hastelloy x plate

,

30mm thickness hastelloy plate

,

hastelloy x plate 30mm thickness

Hastelloy® X is a high temperature and corrosion resistant nickel-based solid solution strengthened alloy. This alloy has outstanding resistance to oxidation and possesses exceptional strength at elevated temperatures. Molybdenum enables this alloy to be hard, strong, and suitable for welding applications. Alloy X exhibits good formability and machinability.

Alloy X is non-magnetic. It has high strength up to 1500ºF (816ºC) and good oxidation resistance up to 2200ºF (1204ºC). This alloy is especially resistant to carburization and nitriding, conditions which cause failure in some high temperature alloys. It is used extensively in high temperature jet engine and chemical processing applications and is highly resistant to stress corrosion cracking in petrochemical applications. Industrial furnace applications incorporate Alloy X for its resistance to oxidizing and its ability to maintain good ductility after prolonged exposure to extremely high temperatures.


 

Alloy X Inventory Size Ranges

Sheet & Coil

0.020" - 0.125"

Sheet | Coil

Plate

0.250" - 3.000"

Bar

0.250" - 6.500"

 


Working with Alloy X nickel

Alloy X materials can be cold rolled to various tempers. It cannot be hardened through heat treating. It is easily fabricated. Alloy X maintains excellent corrosion resistance. It is readily formed by cold-working.

Machining Alloy X nickel

Nickel alloys are stronger at metal cutting temperatures than other materials. Machining of nickel alloys such as Alloy X requires tooling that minimizes cutting forces with maximum edge strength. This alloy exhibits good ductility after prolonged temperatures up to 1600°.

Purchasing Alloy X nickel in sheet, coil, round bar, and plate

We are suppliers of Alloy X nickel in sheet, coil, round bar, and plate stock in a variety of lengths and widths, and we can custom cut this material to your exact specifications. Our nickel coil can also be slit to your desired width.

Not finding what you are looking for Connect with our sourcing group at


Not finding what you are looking for? Connect with our sourcing group


Standard Inventory Specifications

Alloy X Sheet, Coil and Plate:

AMS 5536

ASTM B 435

Alloy X Bar:

AMS 5754

ASTM B 572


Other industry standards we comply with:

ASME SB 435

EN 2.4665

B50A249C

B50A436

B50A463

PWA-LCS

GE Aircraft Engine (GT193)

GE Aviation S-SPEC-35 AeDMS S-400

RR SABRe Edition 2

DFARS Compliant


Common Trade Names

Inconel HX® Special Metals

Hastelloy X® Haynes International

ATI HX ™ Allegheny Technologies

Alloy-X


Common Applications of Alloy X

Jet engine components

Afterburners

Tailpipes

Gas turbine operations

Petro-chemical

Structural components

Industrial furnace

Flash drier components

 

 

Alloy X Chemical Composition
  Element Percent by Weight
C Carbon 0.05 - 0.15
Mn Manganese 1.00 maximum
P Phosphorus 0.040 maximum
S Sulfur 0.030 maximum
Si Silicon 1.00 maximum
Cr Chromium 20.50 - 23.00
Ni Nickel Balance
Mo Molybdenum 8.00 - 10.00
Ti Titanium 0.15 maximum
Al Aluminum 0.50 maximum
Co Cobalt 0.50 - 2.50
B Boron 0.01 maximum
Cu Copper 0.50 maximum
W Tungsten 0.20 - 1.00
Fe Iron 17.00 - 20.00

 

Alloy X Physical Properties

Density: 0.297 lb/in3 (8.22 g/cm3

Specific Gravity: 8.22

Melting Range: 2300 - 2470°F (1260 - 1355°C)

Magnetic Permeability: < 1.002

Thermal Conductivity

Temperature Range Coefficients
°C °F W/m·K Btu/(hr/ft²/in/°F)
21 70 9.1 5.23
93 200 11.0 6.33
260 500 14.1 8.17
593 1100 20.8 12.0
704 1300 22.9 13.2
816 1500 25.0 14.5
927 1700 27.2 15.7

Electrical Resistivity

Temperature microhm-cm
°C °F
21 70 115.8
200 392 120
400 752 123
500 1112 127
800 1472 128
1000 1832 129

 

Alloy X Mechanical Properties

Mechanical Properties

Temperature 0.2% Yield Strength Ultimate Tensile Strength Elongation Percent
°F °C psi MPa psi MPa
-321 -196 - - 150,200 1035 46
-108 -78 - - 118,800 819 51
72 22 47,000 324 104,500 720 46
400 204 48,700 336 103,400 713 41
600 316 42,600 294 100,200 691 40
800 427 43,700 301 99,700 687 44
1000 538 41,500 286 94,000 648 45
1200 649 39,500 272 83,000 472 37
1400 760 37,800 261 63,100 435 37
1600 871 25,700 177 36,500 252 51
1800 982 16,000 110 22,500 155 45
2000 1093 8,000 55 13,000 90 40
2200 1204 3,700 26 5,400 37 31

Alloy Uns N06002 Hastelloy X Plate 30mm Thickness 0Alloy Uns N06002 Hastelloy X Plate 30mm Thickness 1Alloy Uns N06002 Hastelloy X Plate 30mm Thickness 2

Hot Tags: alloy uns n06002 hastelloy x plate 30mm thickness, China alloy uns n06002 hastelloy x plate 30mm thickness suppliers, SS409 Stainless Steel Welded Pipe, 1 4510 Stainless Steel Patterned Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, Corrugated SS Roof Sheet

Send Inquiry

whatsapp

Phone

E-mail

Inquiry