Alloy 304/304H (UNS S30400/ S30409) Stainless Steel Plate
video

Alloy 304/304H (UNS S30400/ S30409) Stainless Steel Plate

Alloy 304/304H (UNS S30400/ S30409) is a modification of the most widely utilized "18-8" chromium-nickel austenitic stainless steel. The carbon content is controlled in the range of 0.04-0.10% for increased strength at temperatures above 800°F (427°C). It is an economical and versatile corrosion resistant alloy suitable for a wide range of general purpose applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of alloy 304/304h (uns s30400/ s30409) stainless steel plate in China. If you're going to wholesale high quality alloy 304/304h (uns s30400/ s30409) stainless steel plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 304/304H (UNS S30400/ S30409) is a modification of the most widely utilized "18-8" chromium-nickel austenitic stainless steel. The carbon content is controlled in the range of 0.04-0.10% for increased strength at temperatures above 800°F (427°C). It is an economical and versatile corrosion resistant alloy suitable for a wide range of general purpose applications.

 

It is common practice for 304H to be dual certified as 304 and 304H. The high carbon chemistry of 304H enables 304 to meet the mechanical properties and grain size requirements of 304H.

4 336

Property Imperial Units Metric Units
Density 0.285 lbs/in³ 7.90 g/cm³
Specific Heat 0.12 BTU/lb-°F (32 – 212°F) 502 J/kg-K (0 – 100°C)
Modulus of Elasticity 29.0 x 10⁶ psi 200 GPa
Thermal Conductivity 9.4 BTU/hr/ft²/ft/°F (at 212°F) 16.3 W/m-K (at 100°C)
Melting Range 2550 – 2590°F 1398 – 1421°C
Electrical Resistivity 29.1 Microhm-in at 68°F 73 Microhm-cm at 20°C

Alloy 304/304H has general corrosion resistance similar to 304/304L. It resists atmospheric corrosion, as well as, moderately oxidizing and reducing environments. However, because of its high carbon content, Alloy 304/304H is subject to carbide precipitation in the heat affected zone of welds.

 

Alloy 304/304H is non-magnetic in the annealed condition, but can become slightly magnetic as a result of cold working or welding. It can be easily welded and processed by standard shop fabrication practices.

 

Hot Tags: alloy 304/304h (uns s30400/ s30409) stainless steel plate, China alloy 304/304h (uns s30400/ s30409) stainless steel plate suppliers, Stainless Steel 316 316L 316Ti Sheets And Plates, SS410 Stainless Steel Plate, 1 4510 Stainless Steel Patterned Plate, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Corrugated SS Roof Sheet