ABS DNV EH40 Shipbuild Steel Plate , Construction Steel Plate 1500-3000mm Width
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of abs dnv eh40 shipbuild steel plate , construction steel plate 1500-3000mm width in China. If you're going to wholesale high quality abs dnv eh40 shipbuild steel plate , construction steel plate 1500-3000mm width made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ABS DNV EH40 shipbuild steel plate , construction steel plate 1500-3000mm width
Description
| Name: | Ship Steel Plate | Material: | A D E F Grade |
|---|---|---|---|
| Length: | 6-11m | Width: | 1500-2500mm |
| Thickness: | 5-250mm | Type: | Hot Rolled |
| High Light: |
shipping plate,marine steel plate |
||
Specifications
steel ship plate EH40
Thickness:5-250 mm
Width:1500-3000mm
Standard: ABS/KR/CCS/GL/BV/DNV/LR/KDK/NKK/RINA
ABS DNV EH40 shipbuild steel plate, EH40 steel plate,hot rolled steel plate
| Commodity | EH40 ship steel plate: |
| Standard | AISI, ASTM, BS, DIN, GB, JIS |
| Model |
EH40, DH40, AH40, 2HGR50, EH36, EH32, DH36, DH32, AH32,AH36,Q235A/B/D |
| Thickness | 5 to250mm |
| Width | 1500 to 2500mm |
| Length | as per customer's request |
| Application | Mainly used in automotive, appliance, machine, printing, construction and building materials |
|
DNV EH40 extra high Strength Chemical Composition |
|||||||
|
Grade |
The Element Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
NV/EH40 |
0.18 |
0.10-0.50 |
0.9-1.6 |
0.035 |
0.035 |
0.015-0.08 |
|
|
Nb |
V |
Ti |
Cu |
B |
Ni |
Mo |
|
|
0.02-0.05 |
0.05-0.10 |
0.02 |
0.35 |
0.20 |
0.40 |
0.08 |
|
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
DNV EH40 extra high general strength property |
|||||||
|
Grade |
|
|
Mechanical Property |
|
|||
|
Thickness |
Yield |
Tensile |
Elongation |
Degree |
Energy 1 |
Energy 2 |
|
|
NV/EH40 |
mm |
Min Mpa |
Mpa |
Min % |
-40 |
J |
J |
|
t≤50 |
390 |
510-650 |
20% |
27 |
41 |
||
|
50<t≤70 |
390 |
510-650 |
20% |
30 |
45 |
||
|
70<t≤150 |
390 |
510-650 |
20% |
37 |
55 |
||
|
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
|||||||
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate
|
Equivalent steel grade of NV/EH40 |
|||||||
|
ABS |
KR |
LR |
BV |
CCS |
NK |
GL |
RINA |
|
AB/EH40 |
R EH40 |
LR/EH40 |
BV/EH40 |
CCS/EH40 |
K EH40 |
GL-EH40 |
RI/EH40 |
Advantage of us
1, fast deliver
2, good quality
3, cheap price


Hot Tags: abs dnv eh40 shipbuild steel plate , construction steel plate 1500-3000mm width, China abs dnv eh40 shipbuild steel plate , construction steel plate 1500-3000mm width suppliers, SS409 Stainless Steel Welded Pipe, ASTM A240 Grade 431 10mm Stainless Steel Plate, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, 400 2 4360 Alloy Pipe, Corrugated SS Roof Sheet