347 Stainless Steel Alloy Plate
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 347 stainless steel alloy plate in China. If you're going to wholesale high quality 347 stainless steel alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Alloy 347 (S34700) is stabilized stainless steel plate which offers as its main advantage an excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800 to 1500°F (427 to 816°C). Alloy 347 stainless steel plate is stabilized by the addition of columbium and tantalum.
Alloy 347 stainless steel plate is also advantageous for high temperature service because of its good mechanical properties. Alloy 347 stainless steel plate offers higher creep and stress rupture properties than Alloy 304 and, particularly, Alloy 304L, which might also be considered for exposures where sensitization and intergranular corrosion are concerns.

| Property | Value |
|---|---|
| Density | 0.288 lbs/in³ (7.96 g/cm³) |
| Specific Heat | 0.12 BTU/lb-°F (32 – 212°F) / 500 J/kg-°K (0 – 100°C) |
| Modulus of Elasticity | 28.0 x 10⁶ psi (193 GPa) |
| Thermal Conductivity | 133 BTU/hr/ft²/ft/°F (16.3 W/m-°K) at 200°F (100°C) |
| Melting Range | 2550 – 2635°F (1398 – 1446°C) |
| Electrical Resistivity | 72 Microhm-cm at 20°F |
Hot Tags: 347 stainless steel alloy plate, China 347 stainless steel alloy plate suppliers, 400 2 4360 Alloy Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, ASTM A240 Grade 431 10mm Stainless Steel Plate, SS431 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, SS410 Stainless Steel Plate