310 Stainless Steel Plates & Sheets
video

310 Stainless Steel Plates & Sheets

310 Stainless Steel is an austenitic stainless steel. 310 consolidates great weldability and pliability with extraordinary high temperature properties. Containing a high substance of Nickel and Chromium 310 has great consumption resistance, amazing imperviousness to oxidation and quality up to 2100°F. The higher Chromium and Nickel make this a better stainless steel when looked at than 304 or 309. 310 stainless steel comes in the accompanying shapes: round bar, pipe, sheet, plate, tubing and loop.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 310 stainless steel plates & sheets in China. If you're going to wholesale high quality 310 stainless steel plates & sheets made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

310 Stainless Steel is an austenitic stainless steel. 310 consolidates great weldability and pliability with extraordinary high temperature properties. Containing a high substance of Nickel and Chromium 310 has great consumption resistance, amazing imperviousness to oxidation and quality up to 2100°F. The higher Chromium and Nickel make this a better stainless steel when looked at than 304 or 309. 310 stainless steel comes in the accompanying shapes: round bar, pipe, sheet, plate, tubing and loop.

4 287

 

Steel grades AISI310 (1.4840)
Production Cold-rolled
Standard ASTM A240/A480
Thickness Min: 0.4mm Max: 6.0mm
Width 1000mm, 1250mm, 1500mm, 2000mm, Other sizes on request
Finish 2B, BA, MATT, M.PVC, N4, N5, SB, HR, N8, Oil base wet polished, Both sides polished available
Coating PVC coating normal/laser
Film: 100 micrometer
Color: black/white
Package weight 1.0-2.2 tonnes
Application Medical equipment, Food industry, Construction material, Kitchen utensils, BBQ grill, Building construction, Electric equipment,

Hot Tags: 310 stainless steel plates & sheets, China 310 stainless steel plates & sheets suppliers, ASTM A240 Grade 409L 3 0 40 0mm Hot Rolled Stainless Steel Plate, SS410 Stainless Steel Plate, SS409 Stainless Steel Welded Pipe, Stainless Steel 316 316L 316Ti Sheets And Plates, 1 4510 Stainless Steel Patterned Plate, 400 2 4360 Alloy Pipe