STM B861 Square Welded Titanium Pipe
video

STM B861 Square Welded Titanium Pipe

Model NO. Titanium Pipe Technique Hot Rolled Grade GR7 Shape Square Model Number Titanium Tube Cerficication En10204-3.1b Surface Pickled, Polished Condition Annealed
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stm b861 square welded titanium pipe in China. If you're going to wholesale high quality stm b861 square welded titanium pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

STM B861 Square Welded Titanium Pipe

Grade5 Titanium welded pipe as per ASME SB861 from 6mm OD to 700mm

AVAILABLE SIZES
Welded: from 6mm OD to 700mm
Seamless: from 5mm OD to 168mm, up to 18mtrs length
*Special seamless Pipes and tubes in bigger or smaller diameter are available upon request.

PROCESSING
Cold rolling, Extruding, Welding, Hot Expanding

STANDARD
ASME SB861, ASME SB338, ASME SB337, DIN 17861, AMS4943, AMS 4944, AMS 4945, etc.


EXAMPLE APPLICATIONS
Funny car body trees, golf clubs, heat exchangers, hydraulic lines, wheelchairs, chemical plants, oil and gas production, tennis rackets, lacrosse sticks, drive shaft tunnel supports, exhaust tubing, wheelie bars, suppressors, heat exchangers

STANDARD CHEMICAL COMPOSITION (weight %, max or range) MECHANICAL PROPERTIES (min)
ASTM B862 UNS
No
N C H Fe O Al V Pd Mo Ni Tensile Yield El. Red.
Mpa Mpa % %
GR 1 R50250 0.03 0.08 0.015 0.2 0.18           240 138 24 30
GR 2 R50400 0.03 0.08 0.015 0.3 0.25           345 275 20 30
GR 3 R50550 0.05 0.08 0.015 0.3 0.35           450 380 18 30
GR 4 R50700 0.05 0.08 0.015 0.5 0.4           550 483 15 25
GR 5 R56400 0.05 0.08 0.015 0.4 0.2 5.5-6.75 3.5-4.5       895 828 10 25
GR 7 R52400 0.03 0.08 0.015 0.3 0.25     0.12-0.25     345 275 20 30
GR 9 R56320 0.03 0.08 0.015 0.25 0.15 2.5-3.5 2.0-3.0       620 483 15 25
GR 12 R53400 0.03 0.08 0.015 0.3 0.25       0.2-0.4 0.6-0.9 483 345 18 25
GR 23 R56401 0.03 0.08 0.0125 0.25 0.13 5.5-6.5 3.5-4.5       828 759 10 15

Hot Tags: stm b861 square welded titanium pipe, China stm b861 square welded titanium pipe suppliers, SS410 Stainless Steel Pipe, Inconel 625 Alloy Steel Plate, 1 4509 1 4510 Pipes And Tubes, 410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe, 420J1 420J2 316 Stainless Pipe