Stainless Steel Seamless Hydraulic Tube And Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel seamless hydraulic tube and pipe in China. If you're going to wholesale high quality stainless steel seamless hydraulic tube and pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel Seamless Hydraulic Tube and Pipe
Product Description
1) Commodity name: Stainless steel seamless hydraulic tube and pipe
2) Process method: Cold drawn
3) Surface finish: Annealed/pickled
4) Material: TP304, TP304L, TP304/304L, TP310S, TP316, TP316L, TP316/316L, TP317L, TP321, TP347H, S31803, 904L
5) Standards: ASTM (ASME) SA/ A213/ M ASTM(ASME)269 ASTM(ASME)312 JIS G3459 JIS G3463 DIN 17456 DIN 17458 EN10216-5
6) Size:
A) O. D.: Φ 6 to Φ 406mm
B) W.T:1mm to 30mm
7) Length: Max. 13 meters (specific or random)
8) Delivery conditions: Annealed, pickled
Hot Tags: stainless steel seamless hydraulic tube and pipe, China stainless steel seamless hydraulic tube and pipe suppliers, 1 4509 1 4510 Pipes And Tubes, 420J1 420J2 316 Stainless Pipe, Inconel 625 Alloy Steel Plate, Stainless Steel High Pressure Pipe, SS410 Stainless Steel Pipe, 410 Stainless Steel Pipe