Stainless Steel DIN 1.4580 Tubing
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel din 1.4580 tubing in China. If you're going to wholesale high quality stainless steel din 1.4580 tubing made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
The Stainless Steel Din 1.4580 Tubing comprises various metals, including iron, chromium, nickel, and molybdenum. This composition makes the tubing strong and highly resistant to corrosion and rust in multiple environments. With its resistance to staining and strength, this type of steel tubing is ideal for many commercial applications where strength, corrosion resistance, and heat tolerance are essential factors. It also has an extensive temperature range, allowing it to be used in extreme temperatures without losing performance. This makes it one of the most versatile types of steel readily available on the market today.

1.4580 X6CrNiMoNb17-12-2 AISI 316Cb Chemical composition(wt.%)
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
|---|---|---|---|---|
| C | - | 0.080 | ||
| Si | - | 1.00 | ||
| Mn | - | 2.00 | ||
| P | - | 0.045 | ||
| S | - | 0.015 | ||
| Cr | 16.50 | 18.50 | ||
| Mo | 2.00 | 2.50 | ||
| Ni | 10.50 | 13.50 | ||
| Nb | 10×C | 1.00 |
Mechanical properties of grade X6CrNiMoNb17-12-2, 1.4580, AISI 316Cb, UNS S31640 EN 10028-7
Yield Strength,Rp 0.2(MPa)
| Condition | Min | Max | Similar | Note |
|---|---|---|---|---|
| Forgings | 220 | 250 | ||
| Hight temperature 50°C | 207 | |||
| Hight temperature 150°C | 177 |
Tensile Strength,Rm(MPa)
| Condition | Min | Max | Similar | Note |
|---|---|---|---|---|
| Forgings | 520 | 720 | ||
| Hight temperature 50°C | 490 | |||
| Hight temperature 150°C | 410 |
| Condition | Min | Max | Similar | Note |
|---|---|---|---|---|
| Forgings | 40 | |||
| Forgings KV. 20°С | 100 |
Hardness
| Condition | Type | Min | Max | Similar | Note |
|---|---|---|---|---|---|
| Forgings | HBW | 230 |
Customer Visit
The Group adheres to the tenet of "one-stop service, making choices easier" and adheres to the business philosophy of "successful customers, happy employees; embracing change, the most important thing is action", and continues to meet the different needs of global customers in the field of the world's steel supply chain. need. A professional sales team provides customers with first-class services; a strict procurement and quality inspection team carefully selects high-quality raw materials; an advanced science and technology team improves production and reduces costs for customers; an excellent design and processing team strives for excellence. Considerate shipping and logistics team to protect product transportation.

Hot Tags: stainless steel din 1.4580 tubing, China stainless steel din 1.4580 tubing suppliers, 1 4509 1 4510 Pipes And Tubes, Inconel 625 Alloy Steel Plate, SS410 Stainless Steel Pipe, Slip On Flanges, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe
You Might Also Like
Send Inquiry