Stainless Steel 310 Seamless Pipes
video

Stainless Steel 310 Seamless Pipes

Stainless Steel 310 Seamless Pipes are pipes made from high alloy austenitic stainless steel containing 25% chromium and 20% nickel. They are designed to withstand high temperatures and resist oxidation and corrosion. They are commonly used in high-temperature applications, such as furnace components, heat exchangers & kilns, as well as in the chemical processing and oil and gas industries.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 310 seamless pipes in China. If you're going to wholesale high quality stainless steel 310 seamless pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

WHAT IS STAINLESS STEEL 310 SEAMLESS PIPES?
Stainless Steel 310 Seamless Pipes are pipes made from high alloy austenitic stainless steel containing 25% chromium and 20% nickel. They are designed to withstand high temperatures and resist oxidation and corrosion. They are commonly used in high-temperature applications, such as furnace components, heat exchangers & kilns, as well as in the chemical processing and oil and gas industries.

 

WHAT IS THE DIFFERENCE BETWEEN 310 AND 310 AND 310H SEAMLESS PIPES?
The main difference between 310, 310, and 310H seamless pipes is their carbon content and intended use. 310 seamless pipes have a maximum carbon content of 0.25%, while 310S seamless pipes have a lower carbon content of 0.08%. This lower carbon content makes 310 more suitable for high-temperature applications requiring welding. 310H seamless pipes have a higher carbon content of 0.04-0.10%, making them ideal for high-temperature applications.

219 74

Density 8.0 g/cm3
Melting Point 1454 °C (2650 °F)
Tensile Strength Psi – 75000 , MPa – 515
Yield Strength (0.2%Offset) Psi – 30000 , MPa – 205
Elongation 35%