SS202 Stainless Tube Steel
video

SS202 Stainless Tube Steel

SS 202 Tube is a low carbon high alloy solid solution chrome steel. SS 202 tube is widely used in applications wherever the corrosion properties don't seem to be adequate. SS 202 Tube is additionally immune to stress corrosion cracking and crevice corrosion. SS 202 Tube is non-magnetic, and is having high formability, toughness and weldability.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss202 stainless tube steel in China. If you're going to wholesale high quality ss202 stainless tube steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 202 tube is made of grade 202 which is a non - stabilized solid solution chrome steel with low carbon content.

SS 202 Tube is a low carbon high alloy solid solution chrome steel. SS 202 tube is widely used in applications wherever the corrosion properties don't seem to be adequate. SS 202 Tube is additionally immune to stress corrosion cracking and crevice corrosion. SS 202 Tube is non-magnetic, and is having high formability, toughness and weldability.

SS 202 tube contains high amounts of pricey ingredients, like metal and nickel.

SS 202 tube was originally developed to resist environments containing dilute sulphuric acid. SS 202 tube offers great toughness, even all the way down to refrigerant temperatures.

217 05

Material Grade
GRADES TP 202 Stainless Steel Tubes / UNS S20200 / DIN 1.4373
SIZE 1/2" NB to 24" NB
STANDARDS ASTM A213, ASTM A249, ASTM A554, ASTM A269, ASTM A270, ASTM A790, ASTM A789
TYPE Seamless Tubes, Welded Tubes, EFW Tubes, ERW Tubes, Fabricated Tubes, Cold Drawn Welded Tubes (CDW Tubes)
FORM Round Tubes, Square Tubes, Rectangular Tubes, Oval Tubes, Hydraulic Tube, etc.
END Plain End, Treaded, Beveled End
TOLERANCE on Length Commercial Length: 6000mm +/- 30mm
Fix Length: from 1200 mm up to 12000mm with a tolerance up to -0/+ 5mm
FINISH Seamless, Welded, Brushed, Pickled, Solution Annealed and Pickled up to O.D. 219.1mm, Polished Grit 120 - 600, Mirror Polished

Hot Tags: ss202 stainless tube steel, China ss202 stainless tube steel suppliers, SS410 Stainless Steel Pipe, 1 4509 1 4510 Pipes And Tubes, Slip On Flanges, 410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe, Inconel 625 Alloy Steel Plate

Send Inquiry

whatsapp

Phone

E-mail

Inquiry