ASTM A790 UNS S32205 Duplex SS Seamless Pipes
video

ASTM A790 UNS S32205 Duplex SS Seamless Pipes

Grade 2205 stainless steel pipe exhibits excellent corrosion resistance, much higher than that of grade 316. It resists localized corrosion types like intergranular, crevice and pitting. The CPT of this type of stainless pipe is around 35°C. This grade ss pipe is resistant to chloride stress corrosion cracking (SCC) at temperatures of 150°C. Grade 2205 stainless steels are apt replacements to austenitic grades, especially in premature failure environments and marine environments.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm a790 uns s32205 duplex ss seamless pipes in China. If you're going to wholesale high quality astm a790 uns s32205 duplex ss seamless pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Duplex 2205 stainless steel (both ferritic and austenitic) Seamless pipe is used extensively in applications that require good corrosion resistance and strength. The UNS S31803 grade stainless steel has undergone a number of modifications resulting in UNS S32205, and was endorsed in the year 1996. This grade 2205 semless pipe offers higher resistance to corrosion.At temperatures above 300°C, the brittle micro-constituents of this grade undergo precipitation, and at temperatures below -50°C the micro-constituents undergo ductile-to-brittle transition; hence this grade of stainless steel is not suitable for use at these temperatures.

seamless tubeseamless stainless pipe

 

 

Chemical Composition of ASTM A790 UNS S31803 Duplex Stainless Steel Seamless Pipes

 

Grade   C Mn Si P S Cr Mo Ni N
2205 (UNS S31803) Min Max - 0.030 - 2.00 - 1.00 - 0.030 - 0.020 21.0 - 23.0 2.5 - 3.5 4.5 - 6.5 0.08 - 0.20
2205 (UNS S32205) Min Max - 0.030 - 2.00 - 1.00 - 0.030 - 0.020 22.0 - 23.0 3.0 - 3.5 4.5 - 6.5 0.14 - 0.20

 

Mechanical Composition of ASTM A790 UNS S31803 Duplex Stainless Steel Seamless Pipes

 

Grade Tensile Strength
(MPa) min
Yield Strength
0.2% Proof
(MPa) min
Elongation
(% in 50mm) min
Hardness
Rockwell C (HR C) Brinell (HB)
UNS S31803 / 2205 621 448 25 31 max 293 max

 

Physical Properties OF ASTM A790 UNS S31803 Stainless Duplex Seamless Pipes

 

Grade Density
(kg/m3)
Elastic
Modulus(GPa)
Mean Co-eff of Thermal
Expansion (μm/m/°C)
Thermal
Conductivity (W/m.K)
Specific
Heat
0-100°C( J/kg.K)
Electrical
Resistivity
(nΩ.m)
0-100°C 0-315°C 0-538°C at 100°C at 500°C
UNS S31803 / 2205 782 190 13.7 14.2 - 19 - 418 850

 

Customer Visit 

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

 

gnee steelgnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: astm a790 uns s32205 duplex ss seamless pipes, China astm a790 uns s32205 duplex ss seamless pipes suppliers, Slip On Flanges, SS410 Stainless Steel Pipe, Inconel 625 Alloy Steel Plate, 410 Stainless Steel Pipe, 420J1 420J2 316 Stainless Pipe, 1 4509 1 4510 Pipes And Tubes

Send Inquiry

whatsapp

Phone

E-mail

Inquiry