ASME B16.9 Bends Carbon Steel A234 WPB / A333 GR6 / A106 GRB-BG Cryogenic Tube
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of asme b16.9 bends carbon steel a234 wpb / a333 gr6 / a106 grb-bg cryogenic tube in China. If you're going to wholesale high quality asme b16.9 bends carbon steel a234 wpb / a333 gr6 / a106 grb-bg cryogenic tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
ASME B16.9 Bends Carbon Steel A234 WPB / A333 GR6 / A106 GRB-BG Cryogenic Tube
Description
| Certification: | CE, ISO, BV, SGS | Product Name: | Carbon Steel A333 GR6 Cryogenic Tube |
|---|---|---|---|
| OD: | 12mm-620mm | Wall Thickness: | 0.25mm-45mm |
| Length: | 1000mm-12000mm | Shape: | Round |
| Standard: | ASTM, AISI, JIS, DIN, EN, GB | Technique: | ERW |
| Sample: | Allowed | Application: | Machinery |
| High Light: |
carbon steel seamless pipe,heavy steel pipe |
||
ASME B16.9 Bends, Carbon Steel A234 WPB / A333 GR6 / A106 GRB--BG Cryogenic Tube
| Descriptions | Carbon Steel A333 GR6 Cryogenic Tube |
| Structural pipe |
A234, A333 GR6, A106 |
| Liquid pipe | 20# q295b-e, q345b-e |
| High pressure boiler tube |
20G 15MnG 20MnG 15CrMoG, 12Cr1MoVG St35.8, sa106b, sa106c, sa210a, sa210c, A333P2, A333P11, A33P12, A333P22, A33P36, A333P91, A333P92, A335T2, A335T11, A335T12, A335T22, A335T91, A335T23, A335T9 |
| Pipeline |
API SPEC 5L, X42, X52, X60, X65,X70,X80 ASTMA53, ASTM A106, ASTM A333, BS301, BS3602, BS3603, BS3604, PSL1, PSL2, DNV-OS-F101, CSA-Z245 |
| Alloy pipe | 4140, 42CrMo, 32CrMo, 15CrMo, |
| Packing | Black paint, Varnish painting, Tarpaulin packing |
| End | Common round end, beveled. |
| Processing | Galvanizing; cutting; making thread outside the pipe; Machining. |
Production Description
1) Precision pipe Images, Usage and Standard



Usage: Hydraulic Pipe, Fluid Pipe, physical construction, hydraulic device, automobile parts, Steel sleeve, bearing, hydraulic cylinder, Pneumatic cylinder and hydraulic pipe
Standard: ISO, JIS, GB, DIN, ASTM, API
2) Chemical composition
Chemical composition of precision pipe in frequently used grade
| Standard | Grade | Chemical composition (%) | ||||||||||||
| C | Si | Mn | S | P | Cr | |||||||||
| GB/T699 | 10# | 0.07~0.13 | 0.17~0.37 | 0.35~0.65 | ≤0.035 | ≤0.035 | ||||||||
| GB/T3639-2000 | 20# | 0.17~0.23 | 0.17~0.37 | 0.35~0.65 | ≤0.035 | ≤0.035 | ||||||||
| GB3077-88 | 35# | 0.32~0.39 | 0.17~0.37 | 0.35~0.65 | ≤0.035 | ≤0.035 | ||||||||
| 45# | 0.42~0.50 | 0.17~0.37 | 0.50~0.80 | ≤0.035 | ≤0.035 | |||||||||
| 40cr | 0.37~0.44 | 0.17~0.37 | 0.50~0.80 | ≤0.035 | ≤0.035 | 0.08~1.10 | ||||||||
| 25Mn | 0.22~0.29 | 0.17~0.37 | 0.70~1.00 | ≤0.035 | ≤0.035 | ≤0.25 | ||||||||
| 37Mn5 | 0.30~0.39 | 0.15~0.30 | 1.20~1.50 | ≤0.015 | ≤0.020 | |||||||||
3) Mechanical properties
Mechanical properties of common precision pipe
| Standard | Grade | Designation (%) | ||||||||||||
| Cold finished (hard)(BK) | Cold finished (Soft) BKW | |||||||||||||
| UTS(Ultimate Tensile Strength) | percentage elongation after fracture | UTS(Ultimate Tensile Strength) | percentage elongation after fracture | |||||||||||
| σ b (Mpa) | δ 5(%) | σ b (Mpa) | δ 5(%) | |||||||||||
| GB/T3639-2000 | 10# | ≥410 | ≥6 | ≥375 | ≥10 | |||||||||
| GB3077-88 | 20# | ≥510 | ≥5 | ≥450 | ≥8 | |||||||||
| 35# | ≥590 | ≥4 | ≥550 | ≥6 | ||||||||||
| 45# | ≥645 | ≥4 | ≥630 | ≥5 | ||||||||||
| 40cr | ≥784 | ≥12 | ||||||||||||
| 37Mn5 | ≥784 | ≥12 | ||||||||||||
Remarks:
Cold Finished (Hard): Tubes do not undergo heat treatment following the final cold forming and, thus, have a rather high resistance to deformation
Cold Finished (Soft): The final heat treatment is followed by cold drawing involving limited deformation. Appropriate further processing allows a certain degree of cold forming (e.g. bending, expanding)
Application Field:
Mechanical processing, machinery manufacturing, automobile
4) Quality Control
A. Advanced Production Equipment
B. Production Flow
C. Skill-full and Qualfied Workers, Training and Testing before Working
D. Strictly Qualtity Control System
5) Packing & Shipping
A) Packing Method
Small size in bundles, big size in bulk, with plastic cap to protect both ends, seaworthy packaging or as per customer's requests.
B) Shipping Way
As per customer's request.
Usually by Sea, by Air, by Train or River-and-Sea Coordinated Transport.
FAQ
Q: What about your payment term?
A: Usually T/T or L/C, 30% deposit and 70% before delivery.
Q: what about your standard delivery date ?
A: 30 days after receiving deposit
Q: How about your capacity ?
A: For steel pipes, 50,000 tons per month, 600,000 tons per year. For pipe fittings, 30,000 tons per year
Q: what about your package ?
A: Usually as per customer's requests.
Common packing information: Small size in bundles, big size in bulk, some sizes with plastic cap to protect both ends, seaworthy packaging.
Q: What is your main market &main customers ?
A: We have 12 years experience on steel pipes & pipe fittings. Our main market includes China, Singapore etc. Main Customers including HYST, Keppel group etc.
Q: If products have some quality problem,how would you deal with?
A: We will responsible for all of our quality problems.
Q: How to get accurate price / quotation from you?
A: Please kindly tell us below details and we'll send our quotation to you ASAP:
1) Pipe's outer diameter
2) Wall thickness
3) Section Shape (round, square etc.)
4) Length for each pipe
5) Steel grade
6) Standard (e.g.: API 5L)
7) Order quantity
8) Designation (BK, BKW etc.)
9) Trade Terms
P.S.: more detailed information you clarified, more exact price we provided.
Hot Tags: asme b16.9 bends carbon steel a234 wpb / a333 gr6 / a106 grb-bg cryogenic tube, China asme b16.9 bends carbon steel a234 wpb / a333 gr6 / a106 grb-bg cryogenic tube suppliers, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe, Slip On Flanges, 1 4509 1 4510 Pipes And Tubes, Inconel 625 Alloy Steel Plate, Stainless Steel High Pressure Pipe