A210 Seamless Boiler Steel Tube
video

A210 Seamless Boiler Steel Tube

A210 seamless boiler steel tubes are specifically designed for high-temperature service in boiler and superheater applications. These tubes are made from carbon-manganese steel, providing high strength and resistance to heat and pressure. They are commonly used in power plants, industrial boilers, and other environments where reliability and durability under extreme conditions are crucial.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of a210 seamless boiler steel tube in China. If you're going to wholesale high quality a210 seamless boiler steel tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

A210 seamless boiler steel tubes are specifically designed for high-temperature service in boiler and superheater applications. These tubes are made from carbon-manganese steel, providing high strength and resistance to heat and pressure. They are commonly used in power plants, industrial boilers, and other environments where reliability and durability under extreme conditions are crucial.

219 161

Table 1: Steel grade and chemical composition:

Grade C Mn P S Si
A-1 ≤0.27 ≤0.93 ≤0.035 ≤0.035 ≥0.10
C ≤0.35 0.29-1.06 ≤0.035 ≤0.035 ≥0.10

Table 2: Mechanical property:

Grade Tensile Strength Mpa/ksi Yield Point (Mpa/ksi) Elongation %
A-1 ≥255/37 ≥415/60 ≥30
C ≥275/40 ≥485/70 ≥30