310S SUS310S Stainless Steel Welded Pipe Stainless Steel Tube ASTM A312 TP310S
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 310s sus310s stainless steel welded pipe stainless steel tube astm a312 tp310s in China. If you're going to wholesale high quality 310s sus310s stainless steel welded pipe stainless steel tube astm a312 tp310s made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
310S SUS310S Stainless Steel Welded Pipe Stainless Steel Tube ASTM A312 TP310S
Description
| Steel Grade: | 310s | Type: | Welded |
|---|---|---|---|
| Welding Line Type: | ERW | Standard: | EN,ASTM,AISI,DIN |
| Application: | Construction,Decoration,Industry,boiler | Shape: | Round.square.Rectangle |
| Surface: | Annealing | Product Name: | Stainless Steel Pipe |
| Thickness: | 0.4-30mm | Material: | Stainless Steel 201/304/316 |
| Length: | 6 Meters Or Customized | Outer Diameter: | 6-630mm |
| Technique: | Seamless/Welded | Price Term: | CIF,FOB,CFR,EX-WORK |
| Trade Terms: | FOB CIF CFR CNF EXWORK | ||
| High Light: |
stainless steel pipe astm,stainless steel pipe welding standards |
||
310S Stainless Steel Welded Pipe SUS310S Stainless Steel Tube ASTM A312 TP310S Pipe
310 Stainless Steel is an austenitic stainless steel. 310 combines good weldability and ductility with great high temperature properties. Containing a high content of Nickel and Chromium 310 has good corrosion resistance, excellent resistance to oxidation and strength up to 2100°F. The higher Chromium and Nickel make this a superior stainless steel when compared to 304 or 309.
Specifications
AMS 5521 & AMS 5651
ASME SA 240, ASME SA 312, ASME SA 479
ASTM A 240, ASTM A 276, ASTM A 276 Condition A, ASTM A 276 Condition S, ASTM A 312, ASTM A 479
UNS S31008, UNS S31009
• Tube hangers for petroleum refining & steam boilers
• Radiant tubes
• Coal internal components
• Thermowells
• Anchor bolts
• Flare tips
• Food processing equipment
310 stainless steel comes in the following shapes: round bar, pipe, sheet, plate, tubing and coil.
Stainless Steel 310 Seamless Tubes Supplier
| STANDARD | UNS | WERKSTOFF NR. |
|---|---|---|
| SS 310 | S31000 | 1.4841 |
| SS 310S | S31008 | 1.4845 |
ASTM A213 TP310 SS Seamless Tube, ASTM A213 TP310s SS Seamless Tube Specification
|
310 Stainless Steel Seamless Pipe, 310S Stainless Steel Seamless Pipe |
||||
|---|---|---|---|---|
|
Material |
Size |
Sch. |
Specification |
Manufacturer |
|
ASTM A213 Stainless Steel 310 Seamless Tube |
15 NB |
Sch. 5s |
ASTM A-213 |
china |
|
ASTM A213 Stainless Steel 310s Seamless Tube
|
15 NB |
Sch. 5s |
ASTM A-213 |
china |



Hot Tags: 310s sus310s stainless steel welded pipe stainless steel tube astm a312 tp310s, China 310s sus310s stainless steel welded pipe stainless steel tube astm a312 tp310s suppliers, 420J1 420J2 316 Stainless Pipe, 410 Stainless Steel Pipe, Slip On Flanges, SS410 Stainless Steel Pipe, Stainless Steel High Pressure Pipe, Inconel 625 Alloy Steel Plate