304, 201, 316, 316L Welded A554 Square Pipe
video

304, 201, 316, 316L Welded A554 Square Pipe

Model NO. 8452 Material Stainless Steel Surface Treatment Polished Usage Machinery Industry Section Shape Square Standard API5l. API5c, ASTM A500, ASTM A554
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 304, 201, 316, 316l welded a554 square pipe in China. If you're going to wholesale high quality 304, 201, 316, 316l welded a554 square pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

304, 201, 316, 316L Welded A554 Square Pipe

 

Product: 304, 201, 316, 316L welded stainless Square Pipe(China)

About us
We have advanced technology of management, we win the trust because of our good quality.
We have clannish conscientious and passionate salesman, we gladden and steady the customers with our best service.
We are pure-hearted and awaiting for your kind attention to our company.

product name 304, 201, 316, 316L welded stainless Square Pipe(CHINA)
size OD(20*20mm-500*500mm)*WT(2mm-20mm)*L(6m-11.8m)
material 304, 201, 316L
standard API5L. API5C, ASTM A500
surface Black Vanished, Galvanized, antirust oil, and etc.
user Construction, water heating, car manufacturing, electrical installation and mining etc.

Chemical Composition:

Grade C ≤ Si ≤ Mn ≤ P ≤ S ≤ Ni ≤ Cr ≤
201 0.12 0.75 7 0.045 0.045 1.00-1.28 13.70-15.70
202 0.15 1 2.25 0.045 0.045 4.07-4.17 14.00-16.00
304 0.08 0.75 2 0.045 0.03 8.00-11.00 18.00-20.00
304L 0.035 0.75 2 0.045 0.03 8.00-13.00 18.00-20.00
309 0.15 0.75 2 0.045 0.03 12.00-15.00 22.00-24.00
310S 0.08 1.5 2 0.045 0.03 19.00-22.00 24.00-26.00
316 0.08 1 2 0.045 0.03 10.00-14.00 16.00-18.00
316L 0.035 0.75 2 0.045 0.03 10.00-15.00 16.00-18.00
321 0.04-0.10 0.75 2 0.045 0.03 9.00-13.00 17.00-20.00
405 0.08 0.75 1 0.045 0.03 0.06 11.5-13.5
409 0.089 1 1 0.045 0.05 0.06 10.50-11.75
410 0.15 0.75 1 0.045 0.03 0.06 11.5-13.5
420 0.16-0.25 1 1 0.04 0.03 0.06 12.00-14.00
430 0.12 0.75 1 0.045 0.03 0.06 16.00-18.00
904L 0.02 1 2 0.045 0.03 23.00-28.00 19.00-23.00