Super Duplex Steel UNS S32750 Angle
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of super duplex steel uns s32750 angle in China. If you're going to wholesale high quality super duplex steel uns s32750 angle made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Super Duplex Steel UNS S32750 Angle
Product Details
Oil and gas industry equipment
Offshore platforms, heat exchangers, process and service water systems, fire-fighting systems, injection and ballast water systems
Chemical process industries, heat exchangers, vessels, and piping
Desalination plants, high pressure RO-plant and seawater piping
Mechanical and structural components, high strength, corrosion-resistant parts
Power industry FGD systems, utility and industrial scrubber systems, absorber towers, ducting, and piping

SUPER DUPLEX STEEL UNS S32750 ANGLE CHEMICAL PROPERTIES:
Typical values (Weight %)
| C | Cr | Ni | Mo | N | Others |
|---|---|---|---|---|---|
| 0.020 | 25 | 7 | 4.0 | .27 | S=0.001 |
SUPER DUPLEX STEEL UNS S32750 ANGLE MECHANICAL PROPERTIES:
| Ultimate Tensile Strength, ksi | 116 min. |
|---|---|
| 0.2% Offset Yield Strength 0.2%, ksi | 80 min. |
| 0.1% Offset Yield Strength 0.2%, ksi | 91 min. |
| Elongation in 2 inches, % | 15 min. |
| Hardness Rockwell C | 32 max. |
| Impact Energy, ft.-lbs. | 74 min. |
Hot Tags: super duplex steel uns s32750 angle, China super duplex steel uns s32750 angle suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle
You Might Also Like
Send Inquiry