430 1.4016 Stainless Steel Sheet
video

430 1.4016 Stainless Steel Sheet

430 ss sheet #4 finish is the brushed finish commonly seen on kitchen appliances and backsplashes. 430 Stainless Steel Sheet #4 finish has a PVC film on one side to help protect against scratching during fabrication and installation. Our 430 stainless steel sheet metal meets the criteria for both the #3 and #4 finish.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 430 1.4016 stainless steel sheet in China. If you're going to wholesale high quality 430 1.4016 stainless steel sheet made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Stainless Steel Sheet 430 is a flat shaped sheet of 430 Stainless Steel Alloy.

430 Stainless Steel Alloy is a ferritic, straight chromium, non-hardenable grade, combining good corrosion resistance and formability characteristics with useful mechanical properties.Its ability to resist nitric acid attack permits its use in specific chemical applications, but automotive trim and appliance components represents its largest fields of application.

-3mm-Thick-Sheet stainlessStainless-Steel-Plate 1

 

 

Common uses of Stainless Steel Sheet 430 include:

  • Automotive Trim
  • Chimney Liners
  • Element Supports
  • Fasteners
  • Lashing Wire
  • Linings for Dish Washers
  • Refrigerator Cabinet Panels
  • Stove Trim Rings

 

1.4016 430 Stainless Plate Detainled Information 

Density: 7.75 g/cm³

Electrical Resistivity: 0.60 x10^-6 Ω .m

Elongation A50 mm: 20 Min %

Melting Point: 1425 - 1510 °C

Modulus of Elasticity: 200 GPa

Proof Stress: 260 Min MPa

Tensile Strength: 450 - 600 MPa

Thermal Conductivity: 23.9 W/m.K

Thermal Expansion: 10.4 x10^-6 /K

 

Customer Visit

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

gnee steelgnee steel

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

 

Hot Tags: 430 1.4016 stainless steel sheet, China 430 1.4016 stainless steel sheet suppliers, Super Duplex Steel UNS S32750 Angle, 310 Butt Weld Flanges

Send Inquiry

whatsapp

Phone

E-mail

Inquiry