Stainless Steel 904L Butt Weld Reducer Fittings
video

Stainless Steel 904L Butt Weld Reducer Fittings

We GNEE Steel Specialist in Stainless Steel 904L Butt weld Pipe Fittings, Our sustainable variety of Steel 904L Fittings, Elbow, Tee, Cross, Reducers, is developed using high quality raw materials and are supplied for several market needs. These 904L Stainless Steel Fittings are available at market leading price.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 904l butt weld reducer fittings in China. If you're going to wholesale high quality stainless steel 904l butt weld reducer fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

904L Stainless Steel Buttweld Pipe Fittings come under the ASTM B366 specification with ASME B16.9 and B16.28 standards. These standards and specification specify pipes of nominal bore sizes ranging from 1/8 inches to 48 inches in diameter for high temperature and corrosion resistant services. 904L Stainless Steel Fittings can be seamless and 100% x-ray welded or fabricated.

reducer ss reducer stainless

 

ASTM A403 / ASME SA403 Stainless Steel Buttweld Fittings Specifications:

Specifications ASTM A403 / ASME SA403
Size 1/8" NB TO 48" NB. (Seamless & 100% X-Ray Welded, Fabricated)
Standards ASME/ANSI B16.9, ASME B16.28, MSS-SP-43
Thickness 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75
Type Seamless, Welded, Fabricated, Cross, Stubend, Reducer, Elbow, Tee, Pipe Cap, Bend, etc.


Stainless Steel 904L Pipe Reducer Fittings Equivalent Grade:

STANDARD UNS WERKSTOFF NR. BS KS AFNOR JIS EN
SS 904L N08904 1.4539 904S13 STS 317J5L Z2 NCDU 25-20 SUS 904L X1NiCrMoCu25-20-5

 

SS 904L Pipe Reducer Chemical Composition

 

Grade Cu Mo C Mn Si Ni P S Cr
SS 904L 1.00 - 2.00 4.00 - 5.00 max 0.020 max 2.00 max 1.00 max 23.00 - 28.00 0.040 max 0.030 max 19.00 - 23.00

Stainless Steel 904L Butt weld Pipe Fittings Mechanical Properties

Density Tensile Strength Elongation Yield Strength (0.2%Offset) Melting Point
7.95 g/cm3 Psi - 71000 , MPa - 490 35 % Psi - 32000 , MPa - 220 1350 °C (2460 °F)

 

customer visit

GNEE Steel is a professional stainless steel supplier, providing high-quality stainless steel pipes, stainless steel coils, stainless steel plates, stainless steel pipe fittings, and other stainless steel products.Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.