ANSI B16.9 SS Pipe 1.4509 1.4510 Reducer
video

ANSI B16.9 SS Pipe 1.4509 1.4510 Reducer

Stainless Pipe Reducers Fittings can be applied to power generation, pharmaceutical, paper and other big and small scale industries. Pipe reducers are widely used to provide the greatest connection flexibility in connecting fractional tubes in a variety of installations.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ansi b16.9 ss pipe 1.4509 1.4510 reducer in China. If you're going to wholesale high quality ansi b16.9 ss pipe 1.4509 1.4510 reducer made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS Pipe Reducers can be applied to power generation, pharmaceutical, paper and other big and small scale industries. Pipe reducers are widely used to provide the greatest connection flexibility in connecting fractional tubes in a variety of installations.1.4510 stainless steel (Grade X3CrTi17) is well suited for cold forming e.g. bending, flanging and deep drawing and is well weldable by all processes except gas welding. It is preferred for use in washing machines, silencers and water boilers.

 

1.4510 Stainless Steel Reducer Applications

Off-Shore Oil Drilling Companies Power Generation Petrochemicals Gas Processing
Specialty Chemicals Pharmaceuticals Pharmaceutical Equipment Chemical Equipment
Sea Water Equipment Heat Exchangers Condensers Pulp & Paper Industry

 

1.4510 Stainless Pipe Reducer Chemical Compositions

Element % Present (in product form)
Carbon (C) 0.03
Silicon (Si) 1.00
Manganese (Mn) 1.00
Phosphorous (P) 0.040
Sulfur (S) 0.015
Chromium (Cr) 17.5 - 18.5
Titanium (Ti) 0.10 - 0.60
Niobium (Nb) (3xC+0.30) to 1.00
Iron (Fe) Balance

SS 1.4510 Reducer Mechanical Properties

(At Room Temperature In Annealed Condition)

  Product Form
Product Form C
Thickness mm Max 8
Yield Strength Rp0.2 N/mm2 Longitudinal 230
Transverse 250
Tensile Strength Rm N/mm2 430 - 640

 

Customer Visit

GNEE Steel is a professional stainless steel supplier, providing high-quality stainless steel pipes, stainless steel coils, stainless steel plates, stainless steel pipe fittings, and other stainless steel products.Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

GNEE STEELGNEE STEEL

 

Hot Tags: ansi b16.9 ss pipe 1.4509 1.4510 reducer, China ansi b16.9 ss pipe 1.4509 1.4510 reducer suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle

Send Inquiry

whatsapp

Phone

E-mail

Inquiry