Stainless Steel 304L Forged Fittings
video

Stainless Steel 304L Forged Fittings

Stainless steel 304L forged fittings are robustly built industrial tools used to connect sections of piping in all kinds of gas, liquid, and steam-based operations. They consist of a base metal that is heated and then carefully shaped into various sizes and shapes such as elbows, tees, reducers, unions, caps, and outlets to facilitate fast connection between pipes.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 304l forged fittings in China. If you're going to wholesale high quality stainless steel 304l forged fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Stainless steel 304L forged fittings are robustly built industrial tools used to connect sections of piping in all kinds of gas, liquid, and steam-based operations. They consist of a base metal that is heated and then carefully shaped into various sizes and shapes such as elbows, tees, reducers, unions, caps, and outlets to facilitate fast connection between pipes. When discussing stainless steel 304L forge fitting, the letter "L" stands for Low Carbon. By utilizing a low carbon content, the mechanical properties of the forging are improved, which increases strength and hardness without compromising an item's overall corrosion resistance.

0917 21

These alloys contain carbon, manganese, phosphorous, sulfur, silicon, chromium, nickel, copper, and molybdenum. In the wire industry, grade 304 stainless steel is mainly used. In the annealed condition, SS 304 forged Fittings are non-magnetic, and in cold work, it is magnetic. SS 304L Forged Fittings has good oxidation resistance to maximum temperature and has good welding characteristics. SS 304 forged fittings are performed well in freshwater applications.

Grade UNS DIN JIS EN BS AFNOR GOST
SS 304 S30400 1.4301 SUS 304 X5CrNi18-10 304S31 Z7CN18-09 08Х18Н10
SS 304L S30403 1.4306 / 1.4307 SUS 304L X2CrNi18-9 / X2CrNi19-11 3304S11 Z3CN18-10 03Х18Н11
Property SS 304 SS 304L
C (%) 0.08 max 0.035 max
Mn (%) 2 max 2.0 max
Si (%) 0.75 max 1.0 max
P (%) 0.045 max 0.045 max
S (%) 0.030 max 0.03 max
Cr (%) 18 – 20 18 – 20
Ni (%) 8 – 11 8 – 13

Mechanical properties of SS 304 Forged Fittings at room temperature are ultimate tensile strength, yield strength, elongation, and hardness. SS 304L Forged Fittings have physical properties such as density, electrical resistivity, specific heat, and thermal conductivity. Our fittings have good corrosion resistance, so these fittings are used in various corrosive environments. Fittings contains high elasticity that make it a choice for many deep drawn, spun, or formed parts. For the hardness of these products, heat treatment is not necessary.

0917 18

The material used in SS 304 forged fittings is Stainless Steel. This alloy also has the corrosion resistance and mechanical properties that can be further enhanced by adding other elements, such as nickel, molybdenum, titanium, niobium, manganese, etc. We maintain the quality of materials; they offer great support and attributes that make our products highly suitable for different industrial applications.

Hot Tags: stainless steel 304l forged fittings, China stainless steel 304l forged fittings suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle

Send Inquiry

whatsapp

Phone

E-mail

Inquiry