Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4564 1.4565 steel pipe reducer in China. If you're going to wholesale high quality 1.4564 1.4565 steel pipe reducer made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

1.4564 (17-7PH stainless steel) reducer , is a precipitation-hardening stainless steel reducer featured with high strength, high hardness, excellent fatigue properties, good corrosion resistance and good formability.1.4564 (17-7PH )stainless steel is the best choice for making springs. It has strong corrosion resistance and high tensile strength. It can reach 2000MPA or higher after aging treatment. The most important thing is that the strength is not weaken during long-term usage. This fatigue resistance is due to the addition of AL as a precipitation hardening effect, making the 1.4564 (17-7ph )stainless steel a semi-austenitic and semi-martensitic stainless steel.

1.4565(Alloy 24) stainless reducer is a nitrogen and molybdenum alloyed austenitic stainless steel, resistant to intergranular corrosion and excellent resistance to pitting, crevice corrosion and stress corrosion cracking in sea water and other corrosive media.

reducerss reducer

 

application:
1. When the flow rate of the fluid in the pipeline changes, such as increasing or decreasing, and the flow rate requirement does not change much, a reducer must be used.
2. At the inlet of the pump, in order to prevent cavitation, a reducer needs to be used.
3. At the joints with instruments, such as flow meters and regulating valves, reducers are also required in order to cooperate with the joints of the instruments.

 

Chemical Composition

Grade Fe% Ni% Cr% C% Mn% Si% P% S% Al%
17-7PH Bal. 6.50-7.75 16.00-18.00 Max 0.09 Max 1.0 Max 1.0 Max 0.035 Max 0.03 0.75-1.50

 

Physical Properties

Condition

Density

kg/m3

Resistivity

μΩ.m

A 7810 0.800
TH1050 7650 0.825
RH950 7650 0.830
CH900 7670 0.838

Mechanical Property

Condition

UTS

MPa

0.2% YS

MPa

Elongation % Hardness
A 893 274 35 B85
TH1050 1370 1280 9 C43
C 1517 1310 5 C43
RH950 1620 1510 6 C48
CH900 1820 1890 2 C49

 

Customer Visit

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

gnee steelgnee steel

 

Hot Tags: 1.4564 1.4565 steel pipe reducer, China 1.4564 1.4565 steel pipe reducer suppliers, Super Duplex Steel UNS S32750 Angle, 310 Butt Weld Flanges

Send Inquiry

whatsapp

Phone

E-mail

Inquiry