S32550 Stainless Steel Angle Stock
video

S32550 Stainless Steel Angle Stock

Alloy 32550 stainless angle is finding many cost effective applications in the chemical, marine, metallurgical, municipal sanitation, plastics, oil and gas, petrochemical, pollution control, wet phosphoric acid, paper making and metalworking industries.Called "super" because it is more alloyed than ordinary stainless steels and has superior corrosion resistance, Alloy 32550is being used in areas where conventional stainless' are inadequate or, at best marginal. One good example s in the paper industry which was hit with an epidemic of corrosion problems when environmental laws forced recycling of process liquids In closed systems, chemicals such as chlorides can build up to highly corrosive concentrations over time. Paper makers have found that ordinary stainless equipment, which had previously given good service, was no longer adequate for many applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of s32550 stainless steel angle stock in China. If you're going to wholesale high quality s32550 stainless steel angle stock made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 32550 ss angle  is a highly alloyed, superduplex (ferrite-austenite) solid solution trengthened alloy, which provides high strength and wear resistance while offering superior corrosion resistance compared to 316 stainless steel. Hot and cold forming can be performed via traditional methods keeping in mind that the alloy is higher strength compared to 316 stainless steel.

ss-316l-angles-500x500stainless-steel-316-angle-250x250

Superior Corrosion Resistance:

Pitting

Crevice Corrosion

Chloride Stress Corrosion Cracking

General Corrosion In Many Environments

Good Ductility

High Strength-To-Weight Ratio

High Fatigue Strength In Marine Environments

Superior Abrasion and Cavitation Erosion Resistance

High Mechanical Strength - (over twice the yield strength of austenitic stainless steels)

Good Fabricability

 

Alloy 32550 ss angle bar

Chemical Requirements

 

Ni

Cr

Mo

Mn

C

Si

Fe

Max

6.5

27.0

3.9

1.50

0.04

1.00

Bal

Min

4.5

24.0

2.9

       

 

Tensile Data

Mechanical Property Requirements

 

Ultimate Tensile

Yield Strength (0.2% OS)

Elong.

R/A

Hardness Brinell

Min

110 KSi

80 KSi

15%

   

Max

       

297

Min

760 MPa

550 MPa

     

Max

         

 

Customer Visit

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.

gnee steelgnee steel

 

 

Hot Tags: s32550 stainless steel angle stock, China s32550 stainless steel angle stock suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle

Send Inquiry

whatsapp

Phone

E-mail

Inquiry