OEM ODM 304 Stainless Steel Seamless Tube / Piping 3mm - 50mm Wall Thickness
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of oem odm 304 stainless steel seamless tube / piping 3mm - 50mm wall thickness in China. If you're going to wholesale high quality oem odm 304 stainless steel seamless tube / piping 3mm - 50mm wall thickness made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
OEM ODM 304 Stainless Steel Seamless Tube / Piping 3mm - 50mm Wall Thickness
Description
| Model Number: | 304 | Type: | Seamless |
|---|---|---|---|
| Thickness: | 0.4-30mm | Shape: | Round Section |
| Technique: | Cold Rolled Hot Rolled | ||
| High Light: |
seamless stainless steel tube,ss seamless pipes |
||
OEM ODM 304 Stainless Steel Seamless Tube / Piping 3mm - 50mm Wall Thickness
| Feature: | A) OEM,ODM orders are accepted; B) Best price; C) High quality; D) Prompt delivery; E) Manufacture according to the sizes and design of customers; F) Best service; G) Certification:ISO9001-2008 Can be bended to different shapes to suit for different designs and modeling in the construction work |
|||||
| Material: | Grade: 304, 304L, 316, 316L, 309S, 310, 201 and 202 stainless steel Different grade can meet different customer's requirement |
|||||
| Product Specs: | A:Round pipe 12,13,14,16,19,25.4,31.8,44.5,50.8,63.5,76.2 B:Rectangular pipe 10x30,10x40,10x50,10x75,10x80,10x90,10x100,20x40,20x80,20x100, 25x38,25x50,25x75 etc. |
|||||
| Size: | 6mm-630mm | |||||
| Thickness: | 0.2mm-50mm | |||||
| Length: | standard is 6M,special length can be customized | |||||
| Chemical Composition | Composition | 201 | 202 | 304 | 316 | 430 |
| C | ≤0.15 | ≤0.15 | ≤0.08 | ≤0.08 | ≤0.12 | |
| Si | ≤1.00 | ≤1.00 | ≤1.00 | ≤1.00 | ≤1.00 | |
| Mn | 5.5-7.5 | 7.5-10 | ≤2.00 | ≤2.00 | ≤1.00 | |
| P | ≤0.06 | ≤0.06 | ≤0.045 | ≤0.045 | ≤0.040 | |
| S | ≤0.03 | ≤0.03 | ≤0.030 | ≤0.030 | ≤0.030 | |
| Ni | 0.8-1.0 | 4-6 | 8-10.5 | 10-14 | ||
| Cr | 16-18 | 17-19 | 18-20 | 16-18 | 16-18 | |
| Finish: | 1.Satin 2.400# 3.600~1000# mirror 4.HL brushed 5.Brushed Mirror(two kinds of finishing for one pipe) |
|||||
| Production Capacity | 500 tons per month | |||||
| Application | decorative /industrial/building material | |||||
| Min.bending radius: | A:38.1~50.8=RX1M B:63.5~76.2=RX1.5-2.5M C:88.9~101.6=RX3-4.5M |
|||||
| Production process: | Turn on the roll -- solder side-forming -- weld -- weld the seam inner&external --polishing&fix melting -- fix the diameter&to be straight -- vortex test -- cuted by saw -- press test -- final test -- package | |||||
| Delivery time | 7-10days after order ,according to customer's order quantity. | |||||
| Packing: | Every tube is sleeved in plastic bag individually, and then 10pcs/bundle or 50 pcs/bundle.We can pack as clients' requirement. | |||||
| Payment Terms: | T/T 30% deposit,70% balance should be paid before shipment;L/C,T/ Tare available | |||||
| Validity: | Valid time is 3 days for price usually. | |||||

Processing: Stainless steel tube
There are high-tech equipments to processing stainless coils and sheets/plates with skilled workers.
Cut to length
Decoiling and slitting
Grinding and brushing
Film protection
Plasma and water jet cutting
Folding and embossing
Packaging details
| Packing details | 250Tons per month |
| Export standard package :bundled wooden box or be required | |
| Port:shanghai | |
| Delivery Time | 15 working days |
| Payment Terms | L/C ,T/T , western union , paypal , alipay |
| Shipping |
DHL , UPS , FEDEX , TNT , EMS , by air , by sea , China post , any way you think is suitable |
Hot Tags: oem odm 304 stainless steel seamless tube / piping 3mm - 50mm wall thickness, China oem odm 304 stainless steel seamless tube / piping 3mm - 50mm wall thickness suppliers, 310 Butt Weld Flanges, Super Duplex Steel UNS S32750 Angle