Type 405 Stainless Steel Seamless Elbow
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of type 405 stainless steel seamless elbow in China. If you're going to wholesale high quality type 405 stainless steel seamless elbow made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Products Description
Type 405 Stainless Steel Weld Fitting
Alloy 405 SS Pipe Fitting is a 12% chromium stainless steel designed to be used in the as-welded condition. Unlike the other grades of 12% chromium stainless, 405 is not vulnerable to extensive hardening through air cooling from high temperatures.
UNS S40500 is composed primarily of chromium and iron with minimal amounts of carbon (0.08%), manganese (1%) and silicon (1%). It also contains trace amounts of phosphorus, sulfur and nitrogen. These elements give 405 stainless steel its corrosion resistance properties as well as its strength and hardness.
Products Properties
Chemical Properties:
The chemical properties of grade 405 stainless steel is presented in terms of its chemical composition as shown below.
| Element | Content (%) |
| Iron, Fe | 85, balanced |
| Chromium, Cr | 11.5 min, 14.5 max |
| Silicon, Si | 1.0 1.0 max |
| Aluminum, Al | 0.1 min, 0.3 max |
| Manganese, Mn | 1.0 max |
| Carbon, C | 0.080 max |
| Nickel, Ni | 0250 max |
| Phosphorous, P | 0.040 max |
| Sulfur, S | 0.030 max |
Mechanical Properties:
The mechanical properties of the annealed grade 405 stainless steel is shown below
| Properties | Measurement | Imperial |
| Tensile strength | 448 MPa | 65000 psi |
| Yield strength (@strain 0.200 %) | 276 MPa | 40000 psi |
| Elongation at break (in 50 mm) | 25.00% | 25.00% |
| Elastic Modulus | 200 GPa | 29007 ksi |
| Poisson's ratio | 0.27 – 0.30 | 0.27 – 0.30 |
Type 405 Stainless Steel Elbow Fitting
Due to its affordability and versatility, stainless steel 405 Stainless Steel Pipe Bend is frequently used in domestic appliances such as washing machines, dishwashers and water heaters, as well as in commercial kitchen equipment like stoves, ovens and fryers. Its corrosion resistance also makes it ideal for use in marine environments – particularly saltwater – where other materials may not stand up to harsh conditions over time. In addition to this, 405 stainless steel can be found in automotive components like exhaust systems due to its ability to withstand extreme temperatures without degrading or corroding too quickly.
Customer Case

FAQ
Q: Can I send samples?
A:Of course, we provide free samples and express delivery to customers all over the world.
Q: Do you provide customized product services?
A:Yes, we can produce according to your specifications and drawings.
Q: Can I visit your factory?
A:Customers from all over the world are welcome to visit our factory.
Q: Can you assist me in importing steel for the first time?
A:Yes, we have freight forwarders who will work with you to arrange shipment.
Q:What is your delivery time?
A:Within 7 working days after receiving the balance payment.
Hot Tags: type 405 stainless steel seamless elbow, China type 405 stainless steel seamless elbow suppliers, Super Duplex Steel UNS S32750 Angle, 310 Butt Weld Flanges
You Might Also Like
Send Inquiry