Sus301 Hard Stainless Steel Coil Strip 5517 3mm Slit Edge 10mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sus301 hard stainless steel coil strip 5517 3mm slit edge 10mm in China. If you're going to wholesale high quality sus301 hard stainless steel coil strip 5517 3mm slit edge 10mm made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Sus301 Hard Stainless Steel Coil Strip 5517 3mm Slit Edge 10mm
Description
| Length: | Customer's Request,in Coil | Grade: | 300 Series |
|---|---|---|---|
| Application: | Construction,Kitchenware,Medical Instruments | Type: | Cold Rolled Coil,Strip |
| Standard: | ASTM,AISI,JIS,DIN,GB | Width: | 10mm-1250mm |
| Surface: | BA,2B,HL,2D | Technique: | Cold Rolled |
| Thickness: | 0.15-3.0mm | Edge: | Mill Edge Slit Edge |
| Price Term: | CIF CFR FOB EX-WORK | ||
| High Light: |
Slit Edge Stainless Steel Coils,Sus301 Stainless Steel Coils 3mm,10mm Stainless Steel 5517 Coils |
||
SUS301 1/4 HARD CRES PER AMS 5517 0.3-3mm Stainless Steel Coil Strip
301 Stainless Steel Strips
ASTM A240 Stainless Steel 301 Strips Supplier, Stainless Steel UNS S30100 Strips Manufacturer, Stainless Steel 301 Strip, UNS S30100 Stainless Steel Strips, ASTM A167 Stainless Steel 301 Strips, Stainless Steel 301 Strips, 301 Stainless Steel Strips, SS UNS S30100 Strips Exporter
Hot Rolled Stainless Steel Strips Stockist, Cold Rolled Stainless Steel Strips Exporter, Hot Rolled 301 Stainless Steel Strips, Stainless Steel 301 Strips manufacturer, ASTM A167 301 Stainless Steel Strips Supplier
MITTEL Steels is one of the most prominent suppliers, exporter, and manufacturer of a comprehensive range of 301 Stainless Steel Strips. We offered these SS 301 Strips in different forms and dimensions as per the client's requirement. These 301 Stainless Steel Strips are similar to carbon steel strips and manufactured through the heat treatment process.
301 Stainless Steel Strip is austenitic steel with excellent corrosion resistance and ability to withstand against the high temperatures. These SS Strips are mainly used in many industries applications due to their good thermodynamic properties like thermal conductivity, specific heat capacity and coefficient of linear expansion.
Non-magnetic Stainless Steel 301 Strips are highly demanded in food industries, cement & gas industries, chemical, electrical generator, shaft, pharmaceuticals and many more. Apart from having non-magnetic properties, the SS 301 Strips offer excellent electromagnetic properties including magnetic permeability, electrical conductivity and Young's Modulus of Elasticity. We provide these strips at a very economical price. These Strips are made from superior quality material and machines. These Strips have high demand in various industries and they are used for a variety of applications.
We have a comprehensive range of SS Strips that are available in Hot Rolled Stainless Steel 301 Strips and Cold Rolled Stainless Steel 301 Strips. Both these strips are manufactured according to Indian as well as International standards.
Stainless Steel 301 Strips , Stainless Steel Strips in Singapore, Stainless Steel Strips Price, Stainless Steel Strips Coils, Stainless Steel UNS S30100 Strips for Door, Stainless Steel for Floor, Flat Stainless Steel Strip, Spring Stainless Steel Strip Manufacturer
301 Stainless Steel Strip Specifications:
| Grades | Stainless Steel J1, J2, J4, 201, 202, 301, 304, 304H, 304L , 309, 309S, 310, 310S, 316, 316L, 316TI, 321, 321H, 347, 409, 410, 410S, 420, 430, 441, 904L |
| Thickness | 0.02mm – 5.0mm |
| Width | 3.2mm – 1500mm |
| Length | AS PER CUSTOMER'S REQUIREMENT |
| Type of Material | STAINLESS STEEL SOFT, DEEP DRAW, EXTRA DEEP DRAW, QUARTER HARD, HALF HARD,FULL HARD. |
| Test Certificate | Yes. |
| Finish | NO.1, 2B, 2D, 2H, 2R, No.4, HAIRLINE, SCOTCH BRITE, SATIN FINISH, NO.8, BA. |
| Make | YONGJIN , BAHRU, POSCO KOREA, POSCO THAINOX, COLUMBUS, ACERINOX, APERAM, TISCO, NISSHIN, NIPPON AND MANY MORE MILLS. |
Chemical Composition of Stainless Steel 301 Strip
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 301 | Min | – | – | – | – | – | 16.0 | 2.00 | 10.0 | – |
| max | 0.08 | 2 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.1 |
ASTM A240 SS 301 Strip Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 301 | 515 | 205 | 35% | 75 | 205 |
Stainless Steel 301 Strip Physical Properties
| Physical Properties (Room Temperature) | ||
| Specific Heat (0-100°C) | 500 | J.kg-1.°K-1 |
| Thermal Conductivity | 14.6 | W.m -1.°K-1 |
| Thermal Expansion | 16.5 | mm/m/°C |
| Modulus Elasticity | 193 | GPa |
| Electrical Resistivity | 7.4 | μohm/cm |
| Density | 7.99 | g/cm3 |
Equivalent Grades of 301 Stainless Steel Strip
| STANDARD | UNS | JIS | WERKSTOFF NR. | AFNOR | BS | GOST | EN |
| SS 301 | S30100 | SUS 301 | 1.4310 | – | – | – | – |
Stainless Steel 301 Strips Updated Price List:
Request the latest 301 Stainless Steel Strips List. Please click on the request a quote button or click here to request the updated price list and ready stock information along with your requirement. Sonic Steel maintains stock of all standard items and can export them at the best price for Stainless Steel 301 Strips.
Industries and applications where our 301 SS Strip is used.
Chemicals, Petrochemicals, Oil & Natural Gas Organization, Fats, Fertilizers, Sugar Mills & Distilleries, Cement Industries, Ship Builders, Paper Industries, Pumps, Automation, Paints, Steel Industries, etc.


Hot Tags: sus301 hard stainless steel coil strip 5517 3mm slit edge 10mm, China sus301 hard stainless steel coil strip 5517 3mm slit edge 10mm suppliers, AISI430 Stainless Steel Foil, 316L Stainless Steel Coil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils
You Might Also Like
Send Inquiry